Inconel 718 Sheet
video

Inconel 718 Sheet

Gnee Steel is a trusted manufacturer and supplier dedicated to providing high-quality Inconel 718 plate products. Inconel 718 plates are one of the most in-demand steel products in the industrial market. These plates and sheets are made from Inconel 718 stainless steel. These plates contain chromium and nickel, giving them enhanced corrosion resistance. They also possess higher tensile and yield strength. They are easy to weld, machine, and forge. They can be easily heat-treated and hardened in high-temperature environments. These plates are known for their high impact strength, tensile strength, and fracture toughness. They offer superior durability and are suitable for a wide range of industrial applications.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 718 sheet in China. If you're going to wholesale high quality inconel 718 sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel 718 Plate description

 

Gnee Steel is a trusted manufacturer and supplier dedicated to providing high-quality Inconel 718 plate products. Inconel 718 plates are one of the most in-demand steel products in the industrial market. These plates and sheets are made from Inconel 718 stainless steel. These plates contain chromium and nickel, giving them enhanced corrosion resistance. They also possess higher tensile and yield strength. They are easy to weld, machine, and forge. They can be easily heat-treated and hardened in high-temperature environments. These plates are known for their high impact strength, tensile strength, and fracture toughness. They offer superior durability and are suitable for a wide range of industrial applications.

 

 

product-1-1

GNEE Inconel 718 Plate

 

Inconel 718 plate is also known as UNS N07718 / W.Nr. 2.4668 nickel alloy plate. We manufacture Inconel 718 nickel alloy plates in various sizes.

 

Inconel 718 is renowned for its exceptional corrosion resistance and extremely high strength at elevated temperatures. It is a nickel-based superalloy widely used in aerospace, petrochemical, shipbuilding, and other industries. Whether in extreme high temperatures or harsh chemical environments, Inconel 718 performs exceptionally well, ensuring the long-term stable operation of equipment and structures.

 

As a commonly used nickel alloy plate product, Inconel 718 plates are manufactured using precision coils through cold rolling, leveling, and shearing processes. The plate thickness is typically less than 5 mm. Compared to Inconel thick plates, these plates have a higher surface finish, making them suitable for applications requiring both functionality and aesthetics.

 

At Gnee Steel, we offer high-quality Inconel 718 plates in various sizes and thicknesses, and provide custom cutting, surface treatment, and global delivery services to meet your specific project needs.

 

Contact now

Alloy 718 Sheet

Alloy 718 Sheet

Inconel 718 Strip

Inconel 718 Strip

AMS 5596 Coil

AMS 5596 Coil

 

Specification Of inconel 718 Plate

 

Specifications : ASTM B670 / ASME SB670, AMS 5596, AMS 5597

Dimensions : ASTM, ASME, and API

Inconel Sheet : thickness range from .008" to .0125"

Inconel Plate : thickness ranges from .0125" to 5.00"

Size : 15NB to 150NB In

Tempers : Annealed, 1/4, 1/2 Hard, 3/4 Hard, Full Hard

Hardness : Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Form : Coils, Foils, Rolls, Plain Sheet, Strip, Flats, Blank (Circle), Ring (Flange) etc.

 

Inconel 718 Plate Specification

 

718 Inconel Sheet Plate Equivalent Grades

STANDARD WERKSTOFF NR. UNS
Inconel 718 2.4668 N07718

 

Chemical Composition of ASTM B670 Inconel 718 Sheet

Grade C Mn Si S Cu Fe Ni Cr
Inconel 718 0.08 max 0.35 max 0.35 max 0.015 max 0.30 max - 50.00 - 55.00 17.00 - 21.00
 

Mechanical Properties of ASME SB670 Inconel 718 Plate

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.2 g/cm3 1350 °C (2460 °F) Psi – 1,35,000 , MPa – 930 Psi – 75,000 , MPa – 482 45 %

 

Inconel 718 Plate Technical Data Sheet

 

Inconel 718 Sheet Sizes

SIZES (INCH) SIZES (mm)
.125" 3.18mm
.134" 3.40mm
.156" 3.96mm
.187" 4.75mm
.250" 6.35mm
.312" 7.92mm
.375" 9.53mm
.500" 12.7mm
.625" 15.9mm
.750" 19.1mm
.875" 22.2mm
1" 25.4mm
1.125" 28.6mm
1.250" 31.8mm
1.500" 38.1mm
1.750" 44.5mm
2" 50.8mm
2.500" 63.5mm
3" 76.2mm

 

ASTM B670 UNS N07718 Sheet thickness

INCONEL 718 PLATE THICKNESS
Inconel 718 SURFACE FINISH WIDTH (MM) THICKNESS (MM)
2D - Cold rolled, pickled, heat treated maximum 1524 0.4 to 6.35
Polished, brushed maximum 1524 0.5 to 4.0
2B - Cold rolled, pickled, heat treated, skin passed maximum 2032 0.25 to 8.0
2R - bright annealed, Cold rolled maximum 1524 0.25 to 3.5
2E - heat treated, Cold rolled, mechanically descaled maximum 2032 0.4 to 8.0
2H - Work hardened maximum 1524 0.4 to 6.35

 

Inconel 718 plates are in stock and available for immediate shipment to meet urgent needs.

 

AMS 5596 Hot Rolled Plate

AMS 5596 Hot Rolled Plate

Inconel 718 Alloy Hot Rolled Plate

Inconel 718 Alloy Hot Rolled Plate

Alloy Inconel 718 Cold Rolled Plate

Alloy Inconel 718 Cold Rolled Plate

Alloy Inconel 718 Clad Plate

Alloy Inconel 718 Clad Plate

Inconel 718 Din 2.4668 Polished Plate

Inconel 718 Din 2.4668 Polished Plate

Astm B670 Inconel Alloy 718 Cold Rolled Sheet

Astm B670 Inconel Alloy 718 Cold Rolled Sheet

 

Products and services offered by Gnee Steel

 

Applications of inconel 718 Plate

 

Oil and gas industry wellhead components:
Gate valves
Throttle valve stems
Fasteners
Packers
Tubing hangers
Downhole equipment
Power generation applications, such as fasteners and turbines
Aerospace components
Nuclear power plant containment vessels
Engineering applications suitable for environments from 750°C to cryogenic temperatures

Applications of Hastelloy C276 round bars

99

Packaging method for Alloy 718 Plate

 

Standard export sea freight packaging:
Waterproof paper wrapping + PVC film + strapping + wooden pallet or wooden crate;
Customized packaging available upon request (logo or other content can be printed on the packaging);
Other special packaging can be designed according to customer requirements;
Both horizontal and vertical placement options are available;
International express delivery: DHL/UPS/FEDEX/EMS and our own dedicated lines;
Air or sea freight;
Shipping port: Shanghai, Ningbo, or as specified by you.

Inconel 718 Sheet testing

 

• Mechanical testing, such as area tensile testing
• Hardness testing
• Chemical analysis – Spectroscopic analysis
• Material composition identification – PMI testing
• Flattening test
• Microscopic and macroscopic testing
• Pitting corrosion resistance test
• Flaring test
• Intergranular corrosion (IGC) test

Inconel 718 Sheet testing

 

Alloy 718 Sheet Price

 

Inconel 718 Plates Description Inconel 718 Plates Price
Inconel 718 Stainless Steel Plates (UNS N07718, 2.4668, ALLOY 718) US $ 985-2499 / Ton
718 Nickel Alloy Steel Plates US $ 800-1448 / Ton
Inconel 718 Alloys Corrosion Resistant Steel Plates US $ 1299-1899 / Ton
Inconel 718 Nickel Plates US $ 40-60 / Kg
1mm Steel Plates Inconel 718 US $ 2000-3000 / Ton
Inconel 718 N07718 4169 2.4668 Sheet / Plates US $ 100-200 / kg
Inconel 718 High Temperature Resistant Steel Plates US $ 1000-2500 / Ton
ASTM 670 Customized Hot Rolled Plates Inconel 718 US $ 1900-2200 / Ton

 

About Gnee Steel

 

 

Inconel 718 Plate supplier

 

About Gnee Steel

Request the latest inconel 718 Plate price list. Please call +8615824687445 or email ss@gneesteel.com for information on available stock and the latest price list for inconel 718 Plate.

 

 

modular-1
Please contact us to get a quick quote for the Inconel 718 Plate you need

We supply these Inconel 718 seamless pipes, welded pipes, resistance welded pipes, and electric fusion welded pipes according to ASTM, ASME, and API standards.

 

FAQ

Q: What are the disadvantages of Inconel 718?

A: Disadvantages and alternatives of Inconel 718

Despite its excellent mechanical properties and corrosion resistance, Inconel 718 also has some disadvantages: Cost: Due to the complex manufacturing process, Inconel 718 is expensive. Difficult to machine: Its high hardness makes material removal difficult and accelerates tool wear.

Q: Does Inconel 718 undergo work hardening?

A: Due to its toughness, low thermal conductivity, and tendency to work harden, Inconel 718 is one of the most difficult materials to machine.

Hot Tags: inconel 718 sheet, China inconel 718 sheet suppliers, inconel alloy valve parts, inconel alloy crankshaft parts, inconel alloy communication system parts, Inconel UNS N06625 Welded Pipe, high nickel corrosion alloys, Inconel 625 Stainless Steel Coil

Send Inquiry

whatsapp

Phone

E-mail

Inquiry