Inconel 600 Sheet
video

Inconel 600 Sheet

Available Formats
GNEE Group offers Nickel Alloy Inconel 600 in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 600 sheet in China. If you're going to wholesale high quality inconel 600 sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel 600 Sheet introduce

600 Inconel Polished Cold Drawn Plate Manufacturer, Inconel 600 Checkered Plate, Inconel Alloy 600 Shim, 600 Alloy Flat Plate, Inconel 600 Hot Rolled Plate, Inconel Alloy 600 Plate Global Supplier

At GNEE group, we develop and maintain quality and innovation through unremitting efforts and quality control and channel them into our products. We offer our customers a quality portfolio of products that help them choose the right products for their industries. We are an ISO 9001: 2015 certified company committed to building and managing a customer-centric business.

We are manufacturers, agents, distributors, suppliers and exporters of Inconel 600 Plates which are corrosion and temperature resistant plates with flexible weldability at different temperatures. Our UNS N06600 Inconel 600 Plates contain nickel and chromium which makes it capable of working at low temperatures and strong and durable.

Inconel 600 Sheet

Inconel 600 sheet600 alloy plate

Inconel 600 (Alloy 600, UNS N06600) Plate/Sheet Description:

Inconel alloy is a family of nickel-chromium superalloys and a trademark of Special Metals Corporation. It is typically used in high-temperature applications. Inconel alloy 600 (UNS N06600) is often used for applications that require resistance to corrosion and heat.

Inconel alloy 600 (UNS N06600) is a nickel-chromium-iron alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress corrosion cracking corrosion by high-purity water, and caustic corrosion.

Other trade names: Alloy 600, UNS N06600, W.NR 2.4816, AWS 010, Nickel 600, Nickelvac 600, Ferrochronin 600

Inconel 600 (Alloy 600, UNS N06600) Plate/Sheet Specification:

Metal Type: UNS N06600
Standard: ASTM B168 AMS 5540 Din 17750

Chemical Composition, %

  C Cr Cu Fe Mg Ni S Si
Max 0.15 17 0.5 10 1   0.015 0.5
Min   14   6   72    

Inconel 600 Sheet, Plate Stock List

ALLOY 600 (75 Ni/16 Cr) Dimension
Strip; cold rolled, annealed 0.10x150 mm x coil, 0.12 kg/m
Strip; cold rolled, annealed 0.40x200 mm x coil, 0.7 kg/m
Sheet; cold rolled, annealed 0.4x914.4 mm x coil, 3.03 kg/m
Sheet; cold rolled, annealed 0.5x1000 mm x coil, 4.14 kg/m
Sheet; cold rolled, annealed 0.7x1000x2000 mm, 13.25 kg/pc
Sheet; cold rolled, annealed 0.8x1219 mm x coil, 8.1 kg/m
Sheet; cold rolled, annealed 1.0x1220 mm x coil, 10.10 kg/m
Sheet; cold rolled, annealed 1.2x1200x3000 mm, 37.8 kg/pc
Sheet; cold rolled, pickled, annealed 1.6x1220x3600 mm, 59 kg/pc
Sheet; cold rolled, annealed 2.0x1200x3000 mm, 62 kg/pc
Sheet; cold rolled, annealed, pickled 2.5x1200x3000 mm, 76 kg/pc
cold rolled, soft annealed, descaled, sheared, tread plate, Checker Plate 3.0x1220x3000 mm, 92 kg/pc
Plate; hot rolled, annealed 4.0x1200x3000 mm, 122 kg/pc
Plate; hot rolled, annealed 5.0x2400x6000 mm, 606 kg/pc
Plate; hot rolled, soft annealed 6.0x2440x6000 mm, 746 kg/pc
Plate; hot rolled, descaled, annealed 8.0x2000x4000 mm, 564 kg/pce
Plate; hot rolled, soft annealed 10.0x2000x4000 mm, 726 kg/pc
Plate; hot rolled, soft annealed 12.0x2000x3000 mm, 616 kg/pc
Plate; hot rolled, annealed 20.0x915x1235 mm, 193 kg/pc

ASTM B168 UNS N06600 Sheet Thickness

SIZES (INCH) SIZES (mm)
.125" 3.18mm
.134" 3.40mm
.156" 3.96mm
.187" 4.75mm
.250" 6.35mm
.312" 7.92mm
.375" 9.53mm
.500" 12.7mm
.625" 15.9mm
.750" 19.1mm
.875" 22.2mm
1" 25.4mm
1.125" 28.6mm
1.250" 31.8mm
1.500" 38.1mm
1.750" 44.5mm
2" 50.8mm
2.500" 63.5mm
3" 76.2mm
Inconel Alloy Sheet Testing

Inconel polishing plate

inconel 600

GNEE Group Factory Environment 

Inconel cold rolled sheet

Inconel rolled plate

FAQ

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.

Hot Tags: inconel 600 sheet, China inconel 600 sheet suppliers, inconel alloy fuel system parts, high temperature alloy, inconel alloy transistor parts, B564 Uns N06625 Material Pipe, inconel alloy spinning process, Inconel Seamless Pipe