Inconel 718 Alloy Seamless Pipe
video

Inconel 718 Alloy Seamless Pipe

Key Properties and Features of Inconel 718 Seamless Pipe:
High Strength: Inconel 718 seamless pipe exhibits high tensile and yield strength, especially at elevated temperatures.
Corrosion Resistance: It exhibits strong resistance to various corrosive environments, including chloride-ion stress corrosion cracking.
High-Temperature Resistance: It maintains its strength and performance at elevated temperatures, making it suitable for aerospace and power generation applications.
Weldability and Formability: Inconel 718 seamless pipe is relatively easy to weld and form into a variety of shapes.
Creep Resistance: It exhibits good creep-rupture properties, which is critical in high-temperature applications.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 718 alloy seamless pipe in China. If you're going to wholesale high quality inconel 718 alloy seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel 718 Seamless Pipe description

Inconel 718 Alloy Seamless Pipe

GNEE Inconel 718 Alloy Seamless Pipe

 

Inconel alloy 718 seamless tubing is a high-performance nickel-chromium alloy known for its exceptional strength, corrosion resistance, and high-temperature performance. It is a versatile material suitable for demanding applications across a wide range of industries, including aerospace, oil and gas, and power generation.

Inconel 718 tubing is a weather-resistant nickel-based alloy designed to exhibit excellent yield strength, tensile strength, and creep strength at temperatures up to 1300°F. Inconel 718 tubing ages during annealing and welding without pulse hardening during heating and cooling. Alloy 718 seamless tubing is also a weather-resistant nickel-chromium alloy containing significant amounts of iron, molybdenum, and niobium, along with smaller amounts of titanium and aluminum. These Inconel 718 seamless tubings offer excellent weldability and resistance to post-weld corrosion. These Inconel 718 tubings are commonly used in chemical processing, liquid-fuel rocket engine components, and atmospheric applications.

Contact now

718 Alloy Seamless Pipe Specification

Specification Of Inconel 718 Seamless Pipe

Seamless Pipe Specifications ASTM B167, B517 / ASME SB167, SB517
Seamless Pipe Size 1 / 8" NB - 24" NB
Welded Pipe Size 1 / 8" NB - 24" NB
EFW Pipe Size 6" NB - 48" NB
Outside Diameter 6.00 mm OD up to 914.4 mm OD, Sizes up to 24" NB available Ex-stock, OD Size Steel Tubes available Ex-stock
Manufacturing Techniques Normalized & as Rolled
Pipe Schedule Thickness Range SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS
Seamless Pipes End Types Plain End, Beveled End, Treaded One End, TBE (Treaded Both Ends)

 

Chemical Composition Inconel 718 Seamless Pipe

Grade C Mn Si Cu S Fe Mo Ni Cr
Inconel 718 0.08 max 0.35 max 0.35 max 0.3 max 0.015 max Bal 2.8 – 3.3 50 – 55 Bal

Mechanical Properties Inconel 718 Seamless Pipe

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.1 g/cm3 1350 °C (2460 °F) Psi – 135,000 , MPa – 930 Psi – 70,000 , MPa – 482 45 %

Dimensions Of Inconel 718 Seamless Pipe

Dimensions Of Inconel 718 Seamless Pipe

Nominal Pipe Size Outside Diameter (mm) Nominal Wall Thickness Schedule
NPS DN OD SCH5s SCHl0s SCH 10 SCH 20 SCH 30 SCH40s SCH STD SCH 40 SCH 60 SCH80s SCH XS SCH 80 SCH 100 SCH 120 SCH 140 SCH 160 SCH XXS
1/8 6 10.3   1.24       1.73 1.73 1.73   2.41 2.41 2.41          
1/4 8 13.7   1.65       2.24 2.24 2.24   3.02 3.02 3.02          
3/8 10 17.1   1.65       2.31 2,31 2.31   3.20 3.20 3.20          
1/2 15 21.3 1.65 2.11       2.77 2.77 2.77   3.73 3.73 3.73       4.78 7.47
3/4 20 26.7 1.65 2.11       2.87 2.87 2.87   3.91 3.91 3.91       5.56 7.82
1 25 33.4 1.65 2.77       3.38 3.38 3.38   4.55 4.55 4.55       6.35 9.09
1 1/4 32 42.2 1.65 2.77       3.56 3.56 3,56   4.85 4.85 4.85       6.35 9.70
1 1/2 40 48.3 1.65 2.77       3.68 3.68 3.68   5.08 5.08 5.08       7.14 10.15
2 50 60.3 1.65 2.77       3.91 3.91 3.91   5.54 5.54 5.54       8.74 11.07
2 1/2 65 73 2.11 3.05       5.16 5.16 5.16   7.01 7.01 7.01       9.53 14.02
3 80 88.9 2.11 3.05       5.49 5.49 5.49   7.62 7.62 7.62       11.13 15.24
3 1/2 90 101.6 2.11 3.05       5.74 5.74 5.74   8.08 8.08 8.08          
4 100 114.3 2.11 3.05       6.02 6.02 6.02   8.56 8.56 8.56   11.13   13.49 17.12
5 125 141.3 2.77 3.40       6.55 6.55 6.55   9.53 9,53 9.53   12.70   15.88 19.05
6 150 168.3 2.77 3.40       7.11 7.11 7.11   10.97 10.97 10.97   14.27   18.26 21.95

Application of Inconel 718 Seamless Pipe

  • product-275-198
    Gnee Steel 
    Engineering
  • product-274-197
    Gnee Steel
    Ship Building
  • product-273-198
    Gnee Steel
    Bridges
  • product-274-198
    Gnee Steel
    Petrochemical industry

Testing of Inconel 718 Seamless Pipe

  • product-275-198
    Gnee Steel
    Expansion test
  • product-276-199
    Gnee Steel
    Dimensional testing
  • product-274-198
    Gnee Steel
    Hardness Test
  • product-274-197
    Gnee Steel
    Nondestructive Testing

Packing of Inconel 718 Seamless Pipe

 

  • product-273-196
    Gnee Steel
    Wooden Boxes
  • product-273-196
    Gnee Steel
    Packing Systems
  • product-272-197
    Gnee Steel
    Wrapping Machine steel pipe
  • product-271-191
    Gnee Steel
    Fasteners Packaging

 

Inconel 718 Alloy Seamless Pipe Surface Treatments

  • Pickling treatment
    Gnee Steel
    Pickling treatment
  • Mirror polishing treatment
    Gnee Steel
    Mirror polishing treatment
  • Polishing treatment
    Gnee Steel
    Polishing treatment
  • Sandblasting treatment
    Gnee Steel
    Sandblasting treatment

Gnee Steel offers four surface finishes for ASME SB167 Inconel 600 boiler tubes: pickling, mirror polishing, polishing, and sandblasting.

Inconel 718 Alloy Seamless Pipe process

  • Annealing process
    Gnee Steel
    Annealing process
  • Hot rolling process
    Gnee Steel
    Hot rolling process
  • Cold drawing process
    Gnee Steel
    Cold drawing process
  • ​​Solution + aging process
    Gnee Steel
    Solution + aging process

Gnee Steel offers the following heat treatments for ASME SB167 Inconel 600 boiler tubes: annealing and solution treatment + aging. Gnee Steel also offers hot working and cold working, namely hot rolling and cold drawing.

About Gnee Steel

Gnee Steel
About Gnee Steel

Gnee Steel is a supplier of Inconel 718 Alloy Seamless Pipe. Our product offerings include seamless pipes (sizes from 4 to 219 mm, thicknesses from 0.5 to 20 mm); welded pipes (sizes from 5.0 to 1219.2 mm, thicknesses from 0.5 to 20 mm); plate (thicknesses from 0.1 to 100 mm, widths from 10 to 2500 mm); strip; alloy round bar (sizes from 3 to 800 mm, diameters from 3 to 800 mm); flat bar (sizes from 2 to 100 mm, thicknesses from 10 to 500 mm); hexagonal bar (sizes from 2 to 100 mm); wire rod; and extruded sections. We partner with steel mills to provide our customers with Alloy 718 that meets or exceeds numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS. Gnee Steel stocks and sells Inconel 718 Alloy Seamless Pipe, pipes, plates, strip, sheets, round bars, flat bars, forging billets, hexagons, wire rod, and extruded shapes. Feel free to contact us for a quote at ss@gneesteel.com

Hot Tags: inconel 718 alloy seamless pipe, China inconel 718 alloy seamless pipe suppliers, inconel alloy decoder parts, inconel alloy union fittings, inconel alloy multiplexer parts, lnconel 601 round bar, inconel alloy camshaft parts, inconel alloy flange fittings

Send Inquiry

whatsapp

Phone

E-mail

Inquiry