Inconel 713c 750 Steel Pipe
video

Inconel 713c 750 Steel Pipe

Inconel713C is a nickel-based precipitation hardening equiaxed crystal casting superalloy, with γ' phase as the precipitation strengthening phase, and the service temperature is below 900°C.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 713c 750 steel pipe in China. If you're going to wholesale high quality inconel 713c 750 steel pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel 713c 750 Steel Pipe

GNEE STEEL COMPANY

Our company is engaged in the production and trade of various Inconel 713c 750 Steel Pipe, high-performance, high-precision special-shaped steel pipes and seamless pipes. We have established business relationships with customers in more than 20 countries and regions. Details such as payment method, delivery time and minimum quantity can be negotiated based on the order.

 

This alloy is suitable for making hot-end rotating and stationary precision castings operating below 900°C, such as turbine blades, guide blades, guides and integrally cast turbines. It has been widely used in the production of turbine blades, guide vanes and integrally cast turbines for aviation, ground and marine gas turbines, integrally cast turbine rotors and guides for aerospace missile engines, as well as diesel and gasoline engine booster turbines and hot extrusion dies.

Inconel 713c 750 Steel Pipe Specification

 

Ni

Fe

C

Cr

Mo

Al

Ti

Nb

Other

Bal.

≤2.5

0.08-0.20

12.0-14.0

3.8-5.2

5.0-6.5

0.5-1.0

1.8-2.8

B 0.05-0.15, Zr 0.05-0.15

Inconel 713c 750 Steel Pipe

Inconel 713c 750 Steel PipeInconel 713c 750 Steel Pipe

Hot Tags: inconel 713c 750 steel pipe, China inconel 713c 750 steel pipe suppliers, inconel alloy camshaft parts, inconel alloy integrated circuit parts, inconel alloy detector parts, inconel tube, Inconel 718 Alloy Plate, inconel alloy receiver parts