Inconel Ma754 Alloy Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel ma754 alloy pipe in China. If you're going to wholesale high quality inconel ma754 alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel Ma754 Alloy Pipe
Inconel MA754 is a high-temperature alloy composed of elements such as nickel, cobalt, chromium, aluminum, titanium, niobium and molybdenum. It is a material with excellent corrosion resistance and high temperature strength and is widely used in aerospace, petrochemical, power generation and other fields.
The chemical composition of Inconel MA754 is as follows (%):
Nickel: 40.0-50.0
Cobalt: 26.0-30.0
Chromium: 18.0-22.0
Aluminum: 3.0-4.5
Titanium: 1.5-3.0
Niobium: 0.5-1.5
Molybdenum: 0.5-1.5
Through the reasonable ratio of these elements, Inconel MA754 has excellent physical properties.
Physical properties:
Density: The density of Inconel MA754 is 8.14g/cm³, which is much higher than the density of general steel, aluminum and other metal materials.
Melting point: The melting point of Inconel MA754 is 1320-1390℃, showing good high temperature stability.
Tensile strength: The tensile strength of Inconel MA754 shows excellent performance at high temperatures, and its tensile strength can reach 220MPa at 1100℃.
Oxidation resistance: Inconel MA754 has good oxidation resistance and can be used at high temperatures for a long time without oxidation, showing good corrosion resistance.
Thermal expansion coefficient: The thermal expansion coefficient of Inconel MA754 shows good stability at high temperatures and can maintain its original size for a long time at high temperatures.
In summary, Inconel MA754 is a very excellent high-temperature alloy with excellent physical properties. It has a wide range of applications, including aerospace, petrochemical, power generation and other important fields.
Hot Tags: inconel ma754 alloy pipe, China inconel ma754 alloy pipe suppliers, inconel alloy compressor parts, inconel alloy thermoforming process, inconel alloy instrumentation parts, inconel alloy heating system parts, alloy pipe, inconel alloy compression molding process
You Might Also Like
Send Inquiry