740H Inconel Stainless Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 740h inconel stainless pipe in China. If you're going to wholesale high quality 740h inconel stainless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
740H Inconel Stainless Pipe
| Properties | Metric | Imperial |
|---|---|---|
| Tensile strength | 1120 MPa | 162000 psi |
| Yield strength (at 0.2%) | 827 MPa | 120000 psi |
| Modulus of elasticity | 205 GPa | 29700 ksi |
| Poissons ratio | 0.284 | 0.284 |
| Elongation at break | 31% | 31% |
| Hardness, Rockwell C | 24 | 24 |