Inconel 601
ASTM Standards:B167, B168, B166, B516, B366, B517, B584
Hardness Range:60-80 Rb
Density: 8.1 g/cm³
Melting Point: 1411°C or 2571°F
Operating Temperature Range: 1600°F–2250°F (870°C–1230°C)
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 601 in China. If you're going to wholesale high quality inconel 601 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel 601 introduce
Inconel 601 is a nickel-chromium-iron alloy with a typical composition of 58–63% nickel, 21–25% chromium, and 1.0–1.7% aluminum, with the balance being iron. Its most notable characteristics are excellent resistance to high-temperature oxidation and thermal cycling at temperatures up to 1150°C; it forms a tightly adherent oxide scale that does not spall even under repeated thermal cycling (spalling resistance).
It also performs well in aqueous corrosive environments, carburizing atmospheres, and sulfur-bearing media, retaining high high-temperature strength and toughness after long-term service at elevated temperatures. The alloy is easy to form, machine, and weld, and is available in product forms such as plate, sheet, round bar/rod, and tubing.
As a reliable Inconel 601 supplier, GNEE STEEL holds complete stock of all common Inconel 601 product forms. We custom-make pipes, sheets, pipe fittings and round bars with tailored machining and surface treatments to fit your project requirements. Scroll down to explore our full product lines one by one.
Inconel 601 Available Shape

Inconel 601Seamless Pipe

Inconel 601 Plate

Inconel 601 Pipe Fitting

Inconel 601 Bar
| Standard | Product Form / Description |
|---|---|
| ASTM B167 | Seamless Pipe & Tube |
| ASTM B906 | Plate & Sheet |
| ASTM B829 | Seamless Pipe & Tube |
| ASTM B366 | Fittings |
| ASTM B166 | Rod & Bar |
| ASTM B168 | Plate & Sheet |
Nickel 601 Alloy Specification
Inconel Alloy 601 Equivalent Grade
| Grade | North America | France | Germany | Japan | European | British | Other Names |
|---|---|---|---|---|---|---|---|
| Inconel 601 | UNS N06601 | AFNOR NC23FeA | WNR/DIN 2.4851 | JIS NCF 601 | EURONORM NiCr23Fe | BS NA 49 | Alloy 601/ Nickel 601 |
Inconel 601 Chemical Properties
| Ni | Cr | Al | C | Mn | S | Si | Cu | Fe | |
|---|---|---|---|---|---|---|---|---|---|
| MIN | 58.000 | 21.000 | 1.000 | - | - | - | - | - | Bal |
| MAX | 63.000 | 25.000 | 1.700 | 0.100 | 1.000 | 0.015 | 0.500 | 1.000 |
Mechanical properties of Inconel 601
| Form and Condition | Tensile Strength | Yield Strength (0.2% Offset) |
Elongation, % |
Hardness, Rb |
||
|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | |||
| ROD and BAR | ||||||
| Hot-Finished | 85-120 | 585-825 | 35-100 | 240-690 | 60-15 | 65-95 |
| Annealed | 80-115 | 550-790 | 30-60 | 205-415 | 70-40 | 60-80 |
| PLATE | ||||||
| Annealed | 80-100 | 550-690 | 30-45 | 205-310 | 65-45 | 60-75 |
| SHEET | ||||||
| Cold-Rolled | 115-190 | 790-1310 | 100-175 | 690-1205 | 20-2 | - |
| Annealed | 85-100 | 585-690 | 30-50 | 205-345 | 55-35 | 65-80 |
| TUBE and PIPE | ||||||
| Cold-Drawn & Annealed | 80-110 | 550-760 | 30-60 | 205-415 | 65-35 | 70-95 |
| ALL FORMS | ||||||
| Solution-Treated | 75-110 | 515-760 | 25-55 | 160-380 | 75-40 | 55-95 |
Inconel 601 Physical Properties
| ensity | lb/in³ | 0.293 |
|---|---|---|
| Mg/m³ | 8.11 | |
| Specific Heat | 70°F, Btu/lb-°F | 0.107 |
| 21°C, J/kg-°C | 448 | |
| Melting Range | °F | 2480-2571 |
| °C | 1360-1411 | |
| Curie Temperature | °F | <-320 |
| °C | <-196 | |
| Permeability | 200 oersted (15.9 kA/m) | |
| 76°F (24°C) | 1.003 |
Inconel 601 Price Per Kg
| Material | Price In INR | Price In USD |
|---|---|---|
| Inconel Alloy 601 | ₹ 5000 - Per kg | $ 62.5 - Per kg |
Nickel Alloy 601 Specifications
Specifications: UNS NO6601, WNR 2.4851, EN NiCr15Fe
ASTM Standards for Inconel 601: B167, B168, B166, B516, B366, B517, B584
Hardness Range: 60-80 Rb
Density: 8.1 g/cm³
Melting Point: 1411°C or 2571°F
Operating Temperature Range: 1600°F–2250°F (870°C–1230°C)
Applications of Inconel 601: Chemical industry, heat treatment industry, aerospace industry, nuclear reactors, containers for processing rosin acid in the papermaking process, containers for processing fatty acids, containers for manufacturing sodium sulfide.
Features of Inconel 601: High corrosion resistance, high oxidation resistance, high strength and good weldability, resistance to chloride stress corrosion cracking, non-magnetic, usable over a wide temperature range.
Testing and Documentation: Mill Test Certificate, EN 10204 3.1, Chemical Composition Report, Mechanical Properties Report, Destructive Testing Report, Non-Destructive Testing Report, PMI Test Report, Visual Inspection Report, Third-Party Inspection Report, NABL Certified Laboratory Report.
Packaging: Wooden crate packaging, bubble wrap packaging, steel strapping, or packaged according to customer requirements.
Applications of inconel 601 Alloy
Oil and gas industry
Power plants
Marine and shipbuilding industry
Refining industry
Petroleum and automotive industry
Pharmaceutical industry
Engineering sector
Engines and turbines
Aerospace industry
Construction industry

Inconel 601 VS Inconel 600 Export Selection Guide
|
Selection Dimension |
Inconel 600 |
Inconel 601 |
Export Scenario Recommendation |
|---|---|---|---|
|
Core Advantage |
Excellent static corrosion resistance |
Super thermal cycling anti-oxidation spalling |
Cyclic temperature equipment priority 601 |
|
High-Temp Working Condition |
≤900℃ static constant temperature |
≤1100℃ frequent temperature fluctuation |
High-temperature furnace flue gas system uses 601 |
|
Medium Adaptability |
Acid, alkali, chloride medium |
Dry heat, oxidation, flue gas medium |
Corrosive liquid medium priority 600 |
|
Cost Performance |
Medium price |
High cost performance for thermal cycling scenarios |
Global thermal engineering bulk order mainstream 601 |
Nickel Based Alloy 601 Packaging
GNEE Group Alloy 601 Product Packaging


inconel Alloy 601 Testing
GNEE Group Nickel Alloy 601 Testing
- 100% dimensional tolerance inspection (ensuring assembly precision)
- Full-batch PMI (Positive Material Identification) spectral analysis (preventing material mix-ups)
- Targeted thermal cycling and oxidation resistance spot checks (key export verification item)
- 100% UT (Ultrasonic Testing) (eliminating internal micro-defects)
- Mechanical property re-testing via sampling (ensuring batch performance consistency)


About Gnee Alloy

Please provide the following key parameters to receive an accurate export quotation and technical compliance report for Inconel 601:
1. Product Type: Pipe/Tube, Sheet, Plate, or Bar + specific dimensions and surface finish
2. Operating Conditions: Continuous operating temperature, thermal cycling frequency, and operating medium
3. Order Requirements: Bulk purchase from stock, custom fabrication, or sample order
4. Certification Requirements: Material Test Certificate (MTC) 3.1/3.2, third-party inspection, and regional certifications
Dedicated Export Services: Free sample testing, free material selection consultation based on operating conditions, free cut-to-length and precision machining, end-to-end logistics tracking, and professional seaworthy, anti-corrosion packaging.
Click to get a quote for Inconel 625 products
FAQ
Q1: What is the biggest advantage of Inconel 601 compared with 310S stainless steel?
310S is prone to oxide layer peeling and rapid failure under repeated cold-hot cycling above 800℃; Inconel 601 forms a tightly attached composite oxide film, with excellent anti-spalling performance, stable long-term operation in thermal cycling environments, and its service life is more than 3 times that of 310S.
Q2: What working conditions are not suitable for Inconel 601?
It is not recommended for long-term strong acid, chloride salt corrosion and aqueous medium corrosion working conditions. For liquid corrosive medium equipment, Inconel 600 or Inconel 625 is more suitable.
Q3: Does Inconel 601 need aging heat treatment after processing?
No aging treatment is required. It is a solid-solution strengthened alloy. Standard solution annealing can maximize its thermal cycling oxidation resistance and ductility, meeting all export project usage standards.
Q4: What core documents can be provided for export customs clearance and project audit?
Free EN10204 3.1 factory MTC report, full PMI spectral test report, high-temperature thermal cycling oxidation test report; optional SGS/TUV 3.2 third-party witnessed inspection report and regional equivalent conformity certificate.
Q5: What is the maximum long-term safe service temperature of Inconel 601?
Long-term stable service temperature ≤1100℃, excellent thermal cycling stability; it is the preferred material for industrial furnaces, flue gas treatment and thermal cycling high-temperature equipment in global export projects.
Hot Tags: inconel 601, China inconel 601 suppliers, inconel alloy timer parts, inconel alloy sensor parts, inconel alloy turbine parts, inconel alloy antenna parts, inconel alloy transformer parts, lnconelx 750 bar
Previous
Inconel 601 Round TubesNext
Inconel 718You Might Also Like
Send Inquiry