Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 600 hot rolled plate in China. If you're going to wholesale high quality inconel 600 hot rolled plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Alloy 600 hot rolled plate description

GNEE Inconel 600 hot rolled plate
Inconel 600 hot-rolled plate is a nickel-chromium alloy plate that is processed at high temperatures to provide excellent resistance to heat, oxidation, and various corrosion conditions, including chloride-ion stress corrosion cracking. Its non-magnetic properties, high strength, and excellent weldability make it widely used in demanding, high-temperature applications in industries such as chemical, aerospace, power generation, and nuclear engineering.
Nickel 600 hot rolled plate Specification
Specification of 600 hot rolled Plate & Sheet
| Category | Specification |
|---|---|
| Size | 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm |
| Thickness | 0.1 mm to 12 mm |
| Standards | ASTM / ASME SB 168 |
| Form | Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange) |
| Finish | Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
| Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard, etc. |
Chemical Composition of Inconel Alloy 600 Sheet & Plate
|
Grade |
C |
Mn |
Si |
S |
Cu |
Fe |
Ni |
Cr |
|
Inconel 600 |
0.15 max |
1.00 max |
0.50 max |
0.015 max |
0.50 max |
6 – 10 |
72.00 min |
14 – 17 |
Mechanical Properties of Inconel 600 Sheet & Plates
|
Density |
Melting Point |
Tensile Strength |
Yield Strength (0.2%Offset) |
Elongation |
|
8.47 g/cm3 |
1413 °C (2580 °F) |
Psi – 95,000 , MPa – 655 |
Psi – 45,000 , MPa – 310 |
40 % |
Inconel 2.4816 Hot Rolled Plate Weight Chart
| Gauge | 8 | 26 | 22 | 16 | 24 | 20 | 11 | 14 | 18 | 12 | 10 | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Inconel 600 sheet | Weight (lb/ft2) | 6.93 | 0.756 | 1.26 | 2.52 | 1.008 | 1.512 | 5.04 | 3.15 | 2.016 | 4.41 | 5.67 |
Application of Nickel Alloy 600 hot rolled plate
Uns N06600 hot rolled plate process
Gnee Steel offers the following Inconel 600 hot rolled plate: annealing and solution treatment + aging. Gnee Steel also offers hot working and cold working, namely hot rolling and cold drawing.
About Gnee Steel

Gnee Steel is a supplier of Inconel 600 hot rolled plate. Our product offerings include seamless pipes (sizes from 4 to 219 mm, thicknesses from 0.5 to 20 mm); welded pipes (sizes from 5.0 to 1219.2 mm, thicknesses from 0.5 to 20 mm); plate (thicknesses from 0.1 to 100 mm, widths from 10 to 2500 mm); strip; alloy round bar (sizes from 3 to 800 mm, diameters from 3 to 800 mm); flat bar (sizes from 2 to 100 mm, thicknesses from 10 to 500 mm); hexagonal bar (sizes from 2 to 100 mm); wire rod; and extruded sections. We partner with steel mills to provide our customers with Alloy 600 that meets or exceeds numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS. Gnee Steel stocks and sells Inconel 600 hot rolled plate, pipes, plates, strip, sheets, round bars, flat bars, forging billets, hexagons, wire rod, and extruded shapes. Feel free to contact us for a quote at ss@gneesteel.com