Incoloy Alloy 909 Pipe

INCOLOY alloy 909 (UNS N19909) is a nickel-iron-cobalt alloy whose outstanding characteristics are a constant low coefficient of thermal expansion, a constant modulus of elasticity, and high strength. The alloy is strengthened by a precipitation-hardening heat treatment made possible by additions of niobium and titanium.Incoloy 909 strip, also called Incoloy 909 belt or Incoloy 909 strapping, is a kind of narrow and long nickel alloy material. Incoloy 909 strip has excellent corrosion resistance, high temperature resistance and fatigue resistance, and it also has good flexibility.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 909 pipe in China. If you're going to wholesale high quality incoloy alloy 909 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Incoloy Alloy 909 pipe is an iron-nickel superalloy pipe, known for its excellent high temperature and corrosion resistance, especially its ability to resist sulfide corrosion in high temperature environments. As a high-performance material, Incoloy Alloy 909 pipe plays an important role in many demanding industrial applications. Chemical composition and performance characteristics
Main ingredients: Incoloy 909 contains a high proportion of nickel and iron, and also adds elements such as cobalt, chromium and molybdenum. The reasonable ratio of these elements gives the alloy excellent resistance to high temperature oxidation and sulfidation corrosion.
High temperature resistance: Incoloy 909 can maintain stability at temperatures up to 1400°F (760°C), suitable for many high temperature application scenarios.
Mechanical properties: Under high temperature conditions, the alloy exhibits good mechanical strength and ductility, is easy to process and shape, and meets the needs of complex industrial design.
Application areas and practical use
Chemical industry: In the chemical process of handling acids and sulfur compounds, it is used to manufacture reactors, heat exchangers and other key equipment, and is widely used due to its excellent corrosion resistance.
Energy industry: In the desulfurization and denitrification systems of coal-fired power stations, it is often used to construct boilers and flue gas ducts due to its resistance to sulfide corrosion.
Aerospace: High-temperature components used in aircraft and rocket engines, such as combustion chambers and turbine parts, benefit from its ability to maintain stable performance under extreme temperatures.
Preparation process and technical requirements
Melting and casting: The use of high-precision melting technology ensures the uniform distribution of alloy elements, which is crucial to ensuring the quality of the final product.
Forming processing: The pipe is formed by forging, cold working, etc., and then undergoes solid solution treatment to optimize its lattice structure and improve corrosion resistance and mechanical strength.

Physical Properties

Density g/cm3 8.19
lb/in.3 0.296
Melting Range °F 2540 - 2610
°C 1395 - 1430

Mechanical Properties

Condition & Size Tensile Strength Yield Strength
(0.2% Offset)
Elongation Reduction of Area Hardness
MPa, min MPa, min %, min %, min HB
Solution Treated ... ... ... ... 277 max
Aging Treated 1172 862 10 15 331min

 

Incoloy Alloy 909 pipeIncoloy Alloy 909 pipeIncoloy Alloy 909 pipe

Hot Tags: incoloy alloy 909 pipe, China incoloy alloy 909 pipe suppliers, inconel alloy mechanical parts, inconel alloy reducer fittings, inconel alloy electrical system parts, 686 718 Inconel Pipe, alloy seamless tubing, inconel alloy oscillator parts