Inconel 600 625 690 Alloy Polished Plate
video

Inconel 600 625 690 Alloy Polished Plate

Available Formats
GNEE Group offers Nickel Alloy Inconel 600 625 690 in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 600 625 690 alloy polished plate in China. If you're going to wholesale high quality inconel 600 625 690 alloy polished plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel 600 625 690 Alloy Polished Plate introduce

 

Inconel 600 is a nickel-chromium alloy known for its exceptional heat and corrosion resistance properties. It comprises nickel, chromium, and iron, with small amounts of other elements. Inconel 600 exhibits excellent resistance to oxidation, scaling, and corrosion in high-temperature environments, making it suitable for a wide range of applications. It maintains its mechanical properties even at elevated temperatures and offers excellent resistance to corrosive environments, including acids, alkalis, and seawater. Inconel 600 is commonly used in aerospace, chemical processing, heat treatment, and other industries where high-temperature performance and corrosion resistance are crucial.
Inconel 625 (AMS 5599, UNS N06625) is a nickel-based superalloy with excellent resistance to oxidation and corrosion. The nickel-chromium matrix of this material is reinforced by the addition of molybdenum and niobium, which is alloyed through solid solution strengthening. This process allows alloy Inconel 625 to maintain high strength and toughness at temperatures ranging from cryogenic up to 1800°F (982°C). It is non-magnetic, austenitic, and displays high tensile strength, fabricability, and brazeability. Due to its high nickel content, this alloy is nearly immune to chloride ion stress-corrosion cracking and pitting, which is commonly found in thin-walled seawater applications like heat exchangers, fasteners, and cable sheathing. We sell alloy 625 materials in sheet, coil, plate and round bar.
Inconel Alloy 690 Sheet & Plate is widely used in various industries due to its excellent properties. The grade is a high chromium nickel based alloy that offers excellent resistance to corrosion and strength in high extensive environment. The alloy is highly preferred by the industries to manufacture the excellent quality of sheets and plates. 690 grades Inconel offers outstanding strength and increased hardness in high elevated temperature condition along with the excellent oxidation resistance. Overall, the grade offers good strength as compared with the Inconel grade alloys.

Inconel 600 625 690 Alloy Polished Plate

Inconel 600 Alloy Polished Plate600 alloy Polished Plate

Inconel 600 Sheets and Plates Specification

Specifications : ASTM B168 / ASME SB168

Width : 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc

Length : 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc

Thickness : 0.3 mm to 120 mm

Hardness : Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Finish : Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Form : Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)

Inconel 600 Sheets & Plates Equivalent Grades

Grade UNS DIN JIS BS GOST AFNOR EN
Alloy 600 N06600 2.4816 NCF 600 NA 13 МНЖМц 28-2,5-1,5 NC15FE11M NiCr15Fe

Inconel Alloy 600 Sheets & Plates Chemical Composition

Grade C Mn Si S Cu Fe Ni Cr
Alloy 600 0.15 max 1.00 max 0.50 max 0.015 max 0.50 max 6.00 – 10.00 72.00 min 14.00 – 17.00

 

ASTM B168 Inconel 625 Sheets, Plates Specification

Specifications : ASTM / ASME SB 168, ASTM / ASME SB 424 , ASTM / ASME SB 443

Standard :ASTM, ASME and API

Size : 0.5 MM TO 200 MM THICK IN 1000 MM TO 2500 MM WIDTH & 2500 MM TO 12500 MM LENGTH

Form : Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange)

Finish : Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Hardness : Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Alloy 625 Chequered Plate Equivalent Grade

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN OR
Inconel 625 2.4856 N06625 NCF 625 NA 21 ХН75МБТЮ NC22DNB4M NiCr22Mo9Nb ЭИ602

Inconel 625 Cold Rolled Sheets Chemical Composition

Grade C Mn Si P S Ni Cr Fe Mo Co Al Ti Nb + Ta
Inconel 625 0.10 max 0.50 max 0.50 max 0.015 max 0.015 max 58.0 min 20.0 – 23.0 5.0 max 8.0 – 10.0 1.0 max 0.40 max 0.40 max 3.15 – 4.15

 

690 Alloy Polished Plate Specification

Specifications ASTM B168 / ASME SB168, AMS 5540
Width 1000mm / 1219mm /1250mm / 1500mm / 2000mm
Length 2000 mm / 2440 mm / 2500 mm / 3000 mm / 6000 mm
Thickness 0.1mm to 12 mm Thk
Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.
Finish Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Form Coils, Foils, Rolls, Plain Sheet, Strip, Flats, Blank (Circle), Ring (Flange) etc.

Inconel 690 Sheet & Plates Equivalent Grades :

STANDARD WERKSTOFF NR. UNS
Inconel 690 2.4642 N06690

Chemical Composition of Inconel Alloy 690 Sheet & Plate

Grade C Mn Si S Cu Fe Ni Cr
Inconel 690 0.05 max 0.5 max 0.5 max 0.015 max 0.5 max 7 - 11 Remainder 27 - 31

 

GNEE Group Factory Environment

Inconel Metal Plate factory

Inconel polishing plate

GNEE Group Product Packaging

Inconel Polished Plate

Inconel Thick Plate

FAQ 

Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Q: Will the Test Certificate meet EN10204 3.1/3.2?
A: We will provide Original Mill Test Certificate certified to EN10204 3.1/3.2 for products in stock or further processing needed.
Q: Once the products received by customer were found not comply with the products or contract demands, what will you do?
A: We will compensate the customer for all the loss without any hesitation.

Hot Tags: Inconel 600 625 690 Alloy Polished Plate, China Inconel 600 625 690 Alloy Polished Plate suppliers, inconel seamless Piping, nickel-based, inconel alloy heating system parts, inconel alloy steel piping, inconel alloy cap fittings, inconel alloy relay parts

Send Inquiry

whatsapp

Phone

E-mail

Inquiry