Alloy Inconel 600 601 Seamless Pipe
video

Alloy Inconel 600 601 Seamless Pipe

Both Inconel 601 seamless pipe and Inconel 600 pipe have good high temperature performance. Among them, Inconel 601 round pipe adds more chromium on the basis of Inconel 600 seamless round pipe. Therefore, the main difference between them is the difference in oxidation resistance. In this article, we will compare the similarities and differences of these two alloys from several aspects.

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy inconel 600 601 seamless pipe in China. If you're going to wholesale high quality alloy inconel 600 601 seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Nickel Inconel 600 601 Pipe Description
Inconel 600 601 Seamless Pipe

 

Gnee Steel Inconel 600 601 Seamless Pipe

Both Inconel 600 Pipe and Inconel 601 Seamless Round Tube are nickel-chromium alloys used in high-temperature and corrosive environments, but there are distinct differences between them. While Inconel 600 is known for its high strength and resistance to stress corrosion cracking, Inconel 601 Alloy Pipe offers excellent oxidation resistance due to its higher chromium and aluminum content. Both Inconel 600 Seamless Pipe and 601 Alloy Pipe belong to the same nickel-chromium-iron alloy family, but there are some differences between them. In order to determine which alloy is best for a specific application, it is crucial to understand the differences between the two alloys in terms of composition, mechanical properties, and corrosion resistance. Let's take a deeper look.

 

GNEE STEEL GROUP supplies Alloy Inconel 600 601 Pipe for you

 

In what form does GNEE supply Inconel 600?
Plates
Plates
Rods
Tubes (welded and seamless)
Fittings
Elbows, tees, short ends, return pipes, caps, crossheads, reducers, fittings, etc.
Wire

PRODUCT FORM SIZE RANGE FROM SIZE RANGE TO
Alloy 600 pipe 0.5 in 8 in
Alloy 600 tube 12 mm 260 mm
Alloy 600 pipe fittings 0.5 in 8 in
Alloy 600 flanges 0.5 in 8 in

 

In what forms does GNEE offer Inconel 601?
Plates
Sheets
Bars
Tubes (welded and seamless)
Fittings
Elbows, tees, nipples, returns, caps, crossheads, reducers, fittings, etc.
Wire

PRODUCT FORM SIZE RANGE FROM SIZE RANGE TO
Alloy 601 pipe 0.5 in 8 in
Alloy 601 tube 12 mm 260 mm
Alloy 601 pipe fittings 0.5 in 8 in
Alloy 601 flanges 0.5 in 8 in
Corrosion Resistant Alloy 600 601 Pipe Specification

Inconel 600 Chemical composition

Ni + Co Cr Fe C Mn S Si Cu

72.0 min

14.0-17.0

6.0-10.0

.15 max

1.00 max

.015 max

.50 max

.50 max

Inconel 601 Chemical composition

Ni Cr Al C Mn Si Fe

61.5

22.5

1.4

.05

.3

.2

14

Inconel 600 Melting Point, Density and Tensile Strength

  Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
600 8.47 g/cm3 1413 °C (2580 °F) Psi – 95,000 , MPa – 655 Psi – 45,000 , MPa – 310 40 %

Inconel 601 pipe Mechanical Properties

Grade Tensile Strength (MPa) min Yield Strength 0.2% Proof (MPa) min Elongation (% in 50mm) min Hardness
Rockwell B (HR B) max Brinell (HB) max
601 Psi – 95,000 , MPa -655 Psi – 45,000 , MPa – 310 40

Ni Alloy Inconel 600 601 Seamless Pipe Surface Treatments

  • Mirror polishing treatment
    Gnee Steel

    Mirror polishing treatment

  • Polishing treatment
    Gnee Steel

    Polishing treatment

  • Sandblasting treatment
    Gnee Steel

    Sandblasting treatment

  • Pickling treatment
    Gnee Steel
    Pickling treatment

Gnee Steel provides four surface treatments for Inconel 600 601 Seamless Pipe alloy seamless pipes: pickling, mirror polishing, polishing and sand blasting.

Ni 600 601 Seamless Pipe production process

  • Solution + aging process
    Gnee Steel

    Solution + aging process

  • Cold drawing process
    Gnee Steel

    Cold drawing process

  • Hot rolling process
    Gnee Steel

    Hot rolling process

  • Annealing process
    Gnee Steel

    Annealing process

Gnee Steel provides the following heat treatments for Ni 600 601 Seamless Pipe: Annealing, Solution + Aging. In addition, Gnee Steel also provides hot working and cold working, i.e. hot rolling and cold drawing. 

nickel based Alloy 600 601 Seamless Pipe packing And Company Environment

nickel based Alloy 600 601 Seamless Pipe Testing And Company Environment 

nickel based Alloy 600 601 Seamless Pipe Packing
nickel based Alloy 600 601 Seamless Pipe Packing
nickel based Alloy 600 601 Seamless Pipe
nickel based Alloy 600 601 Seamless Pipe Company Environment
About Gnee Steel
Gnee Steel

 

About Gnee Steel

Gnee Steel is a supplier of Inconel 600 601 metal Pipe, covering pipes: seamless pipes: size: 4 - 219 mm; thickness: 0.5 - 20 mm; welded pipes: size: 5.0 - 1219.2 mm; thickness: 0.5 - 20 mm, plates: plate thickness 0.1 to 100 mm; plate width 10-2500 mm, strips, alloy round bar size: diameter 3-800 mm;, flat bar size: thickness 2-100 mm; width: 10-500 mm, hexagonal bar size: 2-100 mm;, wire and extruded profiles. We work with steel mills to provide customers with 625 alloy, and its products meet or exceed many leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN and BS standards.
Gnee Steel stocks and sells Inconel 600 601 metal Pipe, Tube, Pipes, Plates, Strips, Plates, Round Bars, Flat Bars, Forged Billets, Hexagons, Wires and Extruded Profiles. Feel free to contact us for a quote at ss@gneesteel.com

Hot Tags: Alloy Inconel 600 601 Seamless Pipe, China Alloy Inconel 600 601 Seamless Pipe suppliers, inconel alloy decoder parts, inconel alloy gasket fittings, Inconel Alloy 706 Pipe, inconel alloy flange fittings, inconel alloy multiplexer parts, inconel alloy steel piping

You Might Also Like

Send Inquiry

whatsapp

Phone

E-mail

Inquiry