ASTM B166 UNS N06600 Bright Round Rod
Diameter (Od):Cold Drawn Bar: 4.76~120mm
Quality and Test:Hardness Test, Bending Test, Hydrostatic etc.
Shaple:Round/Sauqre/Flat/Hexagon
ransport Package:Standard Export Package
Production Capacity:1000ton Per Year
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b166 uns n06600 bright round rod in China. If you're going to wholesale high quality astm b166 uns n06600 bright round rod made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
GNEE is a professional supplier and manufacturer of Inconel alloy, exporting 10,000 tons to foreign markets every year.
UNS N06600 bright alloy rod, also known as Inconel 600 alloy rod, is a high-performance nickel-based alloy.
GNEE supplies UNS N06600 bright annealed alloy rod, which is mainly composed of nickel, chromium and iron elements, and has excellent high temperature strength, corrosion resistance and oxidation resistance. This alloy is suitable for various applications in high temperature and highly corrosive environments. It has satisfactory hot strength and high plasticity below 700℃.
Products Data
Inconel Alloy 600 Round Bars Specification
Specification : ASTM B 166 / ASME SB 166
Size : 5 mm To 500 mm Dia in 100 mm TO 6000 mm Length available with NACE MR 01-75.
Length : 100 mm To 3000 mm Long & Above
Finish : Bright, Polish & Black
Our Inconel 600 Round Bars conforms to NACE MR0175/ISO 15156
Inconel Alloy 600 Round, Bright, Hex, Threaded Bar Chemical Composition
|
Grade |
Ni |
Cr |
Fe |
C |
Mn |
S |
Si |
Cu |
|
Inconel 600 |
72.0 min |
14.0 – 17.0 |
6.0 – 10.0 |
0.15 max |
1.0 max |
0.015 max |
0.5 max |
0.5 max |
600 Inconel Alloy Round Bars Mechanical Properties
|
Density |
Melting Point |
Tensile Strength |
Yield Strength (0.2%Offset) |
Elongation |
|
8.47 g/cm3 |
1413 °C (2580 °F) |
Psi – 95,000 , MPa – 655 |
Psi – 45,000 , MPa – 310 |
40 % |
Products Display
ASTM B166 Inconel 600 Round Rod

Why choosing GNEE
GNEE is currently equipped with more than 10 finishing rolling and drawing production lines and 6 electrolysis equipment. It has introduced foreign advanced equipment such as bright annealing furnaces, straightening machines, internal and external fine polishing machines, ECT eddy current and ultrasonic flaw detectors and other high-end instruments, and is equipped with high-grade dust-free room.
please contact us for a quote! ss@gneesteel.com
PRODUCTS TESTING

GNEE FACTORY ENVIRONMENT

GNEE PACKAGING AND SHIPPING

FAQ
What is your delivery time?
Delivery time primarily depends on your order volume. Typically, we deliver within approximately one month for a standard 40FT container. For in-stock items, shipping can be expedited to just 5 days.
What are your payment terms?
Our standard payment terms are a 30% deposit with the remaining balance against the bill of lading. We also accept L/C.
How can you guarantee the quality of my goods?
We ensure all materials undergo 100% PMI testing and precise measurement before shipping. We welcome third-party inspections and provide the EN10204.3.1B Mill Test Certificate for all materials.
Hot Tags: astm b166 uns n06600 bright round rod, China astm b166 uns n06600 bright round rod suppliers, inconel alloy counter parts, Inconel 718 Alloy Plate, Inconel 686 Flat Bar, inconel tube, inconel alloy modulator parts, inconel alloy diode parts
You Might Also Like