ASTM B166 Inconel 600 Nickel Alloy High-temperature Pipe
1. Corrosion Resistance
N06600 seamless steel pipe has excellent corrosion resistance, resisting attack by a variety of chemical media, including sulfuric acid, hydrochloric acid, nitric acid, hydrofluoric acid, and acetic acid.
2. Mechanical Properties
N06600 seamless steel pipe has excellent mechanical properties, including high strength, high toughness, and high hardness.
3. Thermal Properties
N06600 seamless steel pipe also has excellent thermal properties, with good thermal stability and oxidation resistance.
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b166 inconel 600 nickel alloy high-temperature pipe in China. If you're going to wholesale high quality astm b166 inconel 600 nickel alloy high-temperature pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASTM B166 Inconel 600 Alloy High-temperature Pipe description

GNEE ASTM B166 Inconel 600 Nickel Alloy High-temperature Pipe
Astm B163 Inconel 600 High Temperature Tube is a chromium-nickel alloy designed for use in temperatures up to 2000°F and in cryogenic environments. Due to its nickel content, the alloy resists reducing environments and chloride stress corrosion cracking; due to its chromium content, the alloy resists less severe oxidizing conditions.
UNS N06600 Tubing Schedule Chart
| 1/8" IPS(.405"O. D.) | 3 1/2" IPS( 4.000"O. D.) |
|---|---|
| SCH 40, 80 | SCH 10, 40, 80, 160, XXH |
| 1/4" IPS(.540"O. D.) | 4" IPS(4.500"O. D.) |
| SCH 10, 40, 80 | SCH 10, 40, 80, 160, XXH |
| 3/8" IPS(.675"O. D.) | 5" IPS( 5.563"O. D.) |
| SCH 10, 40, 80 | SCH 10, 40, 80, 160, XXH |
| 1/2" IPS(.840"O. D.) | 6" IPS(6.625"O. D.) |
| SCH 5, 10, 40, 80, 160, XXH | SCH 5, 10, 40, 80, 120, 160, XXH |
| 3/4" IPS(1.050"O. D.) | 8 " IPS(8.625"O. D.) |
| SCH 10, 40, 80, 160, XXH | SCH 5, 10, 40, 80, 120, 160, XXH |
| 1" IPS:(1.315′O. D.) | 10" IPS(10.750"O. D.) |
| SCH 5, 10, 40, 80, 160, XXH | SCH 10, 20, 40, 80 (.500), TRUE 80(.500) |
ASTM B166 600 Nickel Alloy High-temperature Pipe Specification
Alloy 600 Seamless Pipe Chemical Composition
| Grade | C | Mn | Si | Fe | S | Cr | Cu | Ni | |
| Inconel 600 Pipe | min. | – | – | – | 6.0 | – | 14.0 | – | 72.0 |
| max. | 0.15 | 1.0 | 0.5 | 10.0 | 0.015 | 17.0 | 0.5 | – | |
Inconel Astm B163 600 Pipe Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| Inconel 600 Pipe | Psi – 95,000 , MPa -655 | Psi – 45,000 , MPa – 310 | 40 | – | – |
AASTM B166 Inconel 600 High-temperature Pipe Surface Treatments
Gnee Steel offers four surface finishes for ASTM B166 600 Alloy High-temperature Pipe: pickling, mirror polishing, polishing, and sandblasting.
ASTM B166 600 Alloy High-temperature Pipe production process
Gnee Steel offers the following heat treatments for ASTM B166 600 Alloy High-temperature Pipe: annealing and solution treatment + aging. Gnee Steel also offers hot working and cold working, namely hot rolling and cold drawing.
ASTM B166 600 Alloy High-temperature Pipe Testing And Qualification Certificate
GNEE Group ASTM B166 600 Alloy High-temperature Pipe Testing And Qualification Certificate


About Gnee Steel

Gnee Steel specializes in the production of various nickel-based alloys. Gnee Steel's product packaging includes steel strapping: Pipes with an outer diameter of 3 inches or less are typically strapped together with polypropylene film to prevent rust during sea transportation, and then secured with steel strapping. Wooden boxes/crates: Pipes are typically packaged in wooden boxes or crates to protect them during transportation, especially those that are longer or have larger diameters. Seaworthy export packaging: Suppliers typically use standard seaworthy export packaging methods, which may include a variety of materials and techniques to protect the pipes during transportation. Tarpaulin packaging: This prevents rain, seawater, and other external factors from penetrating the export wooden crates during transportation. Gnee Steel specializes in the production and sale of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, power, automotive, and nuclear energy industries, and we can provide customized alloy material solutions based on customer needs. For alloy material pricing inquiries or customized alloy material solutions, please contact us for a quote at ss@gneesteel.com.
Hot Tags: astm b166 inconel 600 nickel alloy high-temperature pipe, China astm b166 inconel 600 nickel alloy high-temperature pipe suppliers, Inconel 825 Astm Standard, inconel alloy terminal parts, inconel alloy jack parts, inconel alloy transistor parts, lnconel 718 alloy, Inconel Alloy 625
You Might Also Like
Send Inquiry