Inconel X-750 Flanges
video

Inconel X-750 Flanges

Available Formats
GNEE Group offers Nickel Alloy Inconel X-750 in a variety of forms, including:
Bars
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel x-750 flanges in China. If you're going to wholesale high quality inconel x-750 flanges made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel X-750 Flanges introduce

X-750 Flanges

X-750 FlangesX-750 Flanges

 

Inconel X-750 flanges are designed for high temperature and high pressure applications requiring resistance to corrosive environments. These flanges are particularly resistant to oxidation, pitting and crevice corrosion and can be used in temperatures ranging from cryogenic to 1100°F. They have good strength properties over a wide range of temperatures while maintaining excellent corrosion resistance.

Inconel Alloy X-750 Flanges Specification

Specifications ASTM B564 / ASME SB564

Dimensions ANSI/ASME B16.5, B 16.47 Series A & B, B16.48, BS4504, BS 10, EN-1092, DIN, etc.

Standard ANSI Flanges, ASME Flanges, BS Flanges, DIN Flanges, EN Flanges, etc.

Size 1/2″NB TO 60″NB

Class / Pressure 150#, 300#, 600#, 900#, 1500#, 2500#, PN6, PN10, PN16, PN25, PN40, PN64 etc.

Flange Face Type Flate Face (FF), Raised Face (RF), Ring Type Joint (RTJ)

Grade X-750 UNS (N07750), DIN (2.4669)

Inconel X-750 Alloy Flanges Equivalent Indian Standard

STANDARD UNS WNR.
Inconel X-750 N07750 2.4669

Inconel X-750 Flanges Chemical Composition

Al C Cr Co Cu Fe Mn Nb Ni Ti S Si
0.40-1.0 .08 max 14.0-17.0 1.00 max 0.50 max 5.0-9.0 1.00 max 0.70-1.20 70.0 min 2.25-2.75 .01 max .50 max

X-750 Flanges Mechanical Properties

Ultimate Tensile Strength .2% Yield Strength Elongation %
1250 MPa, 181000 psi 850 MPa, 123000 psi 30

Inconel Alloy Blind Flange

GNEE Group Factory Environment

Inconel Flanges factory

product-759-759

GNEE Group Product Packaging

Inconel X-750 Flanges packing

Inconel X-750 FlangesInconel X-750 Flanges

FAQ 

Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.
Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, Russia, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.
Q: Can you provide samples?
Answer: Yes. As long as you contact us, we can provide free small samples in stock. Customized samples will take about 5-7 days.

Hot Tags: inconel x-750 flanges, China inconel x-750 flanges suppliers, inconel alloy heating system parts, inconel alloy transmitter parts, inconel alloy compressor parts, inconel alloy vacuum forming process, inconel alloy resin transfer molding process, Inconel X 750

Send Inquiry

whatsapp

Phone

E-mail

Inquiry