Incoloy Alloy 890 Seamless Pipe
video

Incoloy Alloy 890 Seamless Pipe

Incoloy Alloy 890 seamless pipe is a critical material for applications requiring exceptional thermal stability and high-temperature performance, along with resistance to oxidation, carburization, and corrosion. Its unique combination of strength, environmental resistance, and fabricability makes it a preferred choice for industries where materials are subjected to extreme conditions.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 890 seamless pipe in China. If you're going to wholesale high quality incoloy alloy 890 seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

INCOLOY alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with excellent resistance to oxidation, carburization, and sulfidation at temperatures up to 2200°F (1200°C).Alloy 890 offers the high chromium content of alloy 803 along with enhanced properties from additions of silicon, molybdenum, and niobium. Alloy 890 is protected by United States Patent Number 5,873,950 dated February 23, 1999.

Element Content (%)
Nickel, Ni 42.5
Iron, Fe 25.605 - 28.4
Chromium, Cr 25
Silicon, Si 1.8
Molybdenum, Mo 1.5
Manganese, Mn ≤1
Titanium, Ti ≤1
Copper, Cu ≤ 0.75
Niobium, Nb 0.4
Tantalum, Ta 0.2
Carbon, C 0.1
Aluminum, Al 0.1

PHYSICAL PROPERTIES

The following table shows the physical properties of INCOLOY alloy 890.

Properties Metric Imperial
Density 7.94 g/cm3 0.287 lb/in3
Melting point 1309-1383°C 2388-2521°F

MECHANICAL PROPERTIES

The mechanical properties of INCOLOY alloy 890 are displayed in the following table.

Properties Metric Imperial
Tensile strength 62 MPa 8990 psi
Yield strength 44 MPa 6380 psi
Elongation at break 46.50% 46.50%

Incoloy Alloy 890 seamless pipeIncoloy Alloy 890 seamless pipeIncoloy Alloy 890 seamless pipe

Hot Tags: incoloy alloy 890 seamless pipe, China incoloy alloy 890 seamless pipe suppliers, alloy for sensors, alloy for metrology baths, alloy for drills, welded alloy pipe, alloy for biofabrication baths, alloy for detectors

Send Inquiry

whatsapp

Phone

E-mail

Inquiry