Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 864 seamless pipe in China. If you're going to wholesale high quality incoloy alloy 864 seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Incoloy Alloy 864 is a high-performance alloy that combines excellent strength and oxidation resistance at elevated temperatures, making it suitable for applications involving heat and stress. The seamless pipe made from this alloy is particularly well-suited for use in aggressive high-temperature environments, such as those encountered in aerospace, industrial furnaces, and chemical processing.
Characteristics of Incoloy Alloy 864 Seamless Pipe:
High-Temperature Strength: Maintains its mechanical properties even at elevated temperatures, making it ideal for high-temperature applications.
Oxidation Resistance: Exhibits exceptional resistance to oxidation, allowing it to withstand the detrimental effects of prolonged exposure to high temperatures without degradation.
Corrosion Resistance: Demonstrates good resistance to certain types of corrosion, expanding its usability in various harsh environments.
Good Stress-Cracking Resistance: Capable of resisting stress cracking, which is crucial in applications involving fluctuating temperatures and stresses.
Weldability: Can be welded using suitable welding techniques, although precautions must be observed due to its high alloy content.
Physical Properties
| Density | g/cm3 | 8.02 | |
|---|---|---|---|
| lb/in.3 | 0.290 | ||
| Melting Range | °F | 2467 - 2539 | |
| °C | 1353 - 1393 | ||
| Permeability at 200 oersted (15.9 kA/m) | 1.004 | ||
| Electrical Resistivity at 70°F (21°C) | ohm•circ mil/ft | 628 | |
| μΩ•m | 1.04 | ||
Mechanical Properties
| Test Temperature | Hardness | Tensile Strength | Yield Strength | Elongation | Fracture Location | ||
|---|---|---|---|---|---|---|---|
| Rb | ksi | MPa | ksi | MPa | % | ||
| 70°F (20°C) | 82 | 79.9 | 550.9 | 46.1 | 317.9 | 17.4 | Weld |
| 70°F (20°C) | 83 | 80.4 | 554.4 | 45.3 | 312.3 | 18.7 | Weld |
| 800°F (427°C) | N/A | 64.5 | 444.7 | 31.7 | 218.6 | 20.5 | Weld |
| 1000°F (538°C) | N/A | 58.4 | 402.7 | 30.9 | 213.1 | 16.6 | Weld |
| 1200°F (648°C) | N/A | 58.9 | 406.1 | 28.9 | 199.3 | 18.4 | Weld |
| 1400°F (759°C) | N/A | 40.9 | 282.0 | 26.4 | 182.0 | 23.5 | Weld |
| 1600°F (871°C) | N/A | 23.4 | 161.3 | 15.9 | 109.6 | 55.0 | Weld |