Incoloy 825 thin-walled tube
Seamless Tube: OD: 1/2- 16 inches
Wall Thickness: SCH10 to SCH160
Welded Tube: OD: 6.35 - 114.3 mm
Wall Thickness: 0.8 - 12.7 mm
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 825 thin-walled tube in China. If you're going to wholesale high quality incoloy 825 thin-walled tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Incoloy 825 thin-walled tube introduce
Incoloy 825 thin-walled tube


Incoloy 825 Tube Specifications
Sizes: 15 NB to 150 NB IN
Types: Seamless / ERW / Welded / Fabricated / Hollow / LSAW Tubes
Wall Thickness: .035" – .095', (Special Wall Thickness Available)
Specifications: SCH5, SCH10, SCH40, STD, SCH80, SCH160
Surface Treatment: Polished, AP (Annealed and Pickled), BA (Bright and Annealed), MF
Shapes: Round, Square, Rectangular, Hydraulic, Straight or "U" Bend, etc.
Lengths: Single Random, Double Random and Cut Lengths.
Ends: Plain End, Bevel End, Threaded
Incoloy 825 seamless pipe is a nickel-iron-chromium alloy with added molybdenum and copper. Incoloy 825 pipe is used in chemical processing, pollution control equipment, oil and gas well piping, nuclear fuel reprocessing, acid production, and pickling equipment. Incoloy 825 pipe is easier to cold form than stainless steel.
Incoloy 825 seamless pipe is designated UNS N08825 and Werkstoff number 2.4858. Alloy 825 pipe is also known as Incoloy 825 pipe, Inconel 825 pipe, and Nickel Alloy 825 pipe. All Alloy 825 seamless pipe, Alloy 825 pipe, Alloy 825 tube, and Alloy 825 instrument tubing have excellent resistance to reducing and oxidizing acids, stress corrosion cracking, and localized attack such as pitting and crevice corrosion.
Incoloy Alloy 825 Tubes Specifications
|
Specifications |
: |
ASTM B163, B516 / ASME SB163, B516 |
|
Dimensions |
: |
ASTM, ASME and API |
|
Alloy 825 Tubes Size |
: |
6 mm OD x 0.7 mm to 50.8 mm OD x 3 mm thk. |
|
Schedule |
: |
SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
|
Type |
: |
Seamless / ERW / Welded / Fabricated / LSAW Tubes |
|
Form |
: |
Round, Square, Rectangular, Hydraulic Etc |
|
Length |
: |
Single Random, Double Random & Cut Length. |
|
End |
: |
Plain End, Beveled End, Treaded |
Mechanical Properties
| Form and Condition | Tensile Strength | Yield Strength (0.2% Offset) |
Elongation | ||
|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | % | |
| Tubing, Annealed | 112 | 772 | 64 | 441 | 36 |
| Tubing, Cold Drawn | 145 | 1000 | 129 | 889 | 15 |
| Bar, Annealed | 100 | 690 | 47 | 324 | 45 |
| Plate, Annealed | 96 | 662 | 49 | 338 | 45 |
| Sheet, Annealed | 110 | 758 | 61 | 421 | 39 |
GNEE Group Factory Environment
Incoloy 825 tube

GNEE Group Product Packaging
825 thin-walled tube

FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.