Incoloy 800/800H/800HT Pipe Fitting
Excellent resistance to high-purity water corrosion
Excellent resistance to strong alkali corrosion
Good weldability over a wide temperature range
Excellent high-temperature oxidation resistance
Resistance to chloride-induced stress corrosion cracking
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 800/800h/800ht pipe fitting in China. If you're going to wholesale high quality incoloy 800/800h/800ht pipe fitting made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Incoloy 800/800H/800HT Pipe Fitting description
Gnee Steel has become a well-known exporter, supplier, manufacturer, and trader of Incoloy 800, 800H, and 800HT pipe fittings in China, offering a full range of products. These fittings are renowned for their durability, corrosion resistance, excellent bending performance, and robust construction. Durability, solid design, and excellent surface finish are among their many advantages.

GNEE Incoloy 800/800H/800HT Pipe Fitting
Incoloy 800 alloy fittings are an alloy of nickel, iron, and chromium. They maintain their stability and austenitic structure even after prolonged exposure to high temperatures. They exhibit excellent resistance to carburization and oxidation in high-temperature and aqueous environments, while also possessing superior strength. They are typically used in high-temperature applications below 1100°F (593°C).
Incoloy 800H fittings are an iron-nickel-chromium alloy with the same basic composition as Incoloy 800, but with higher creep rupture strength. This enhanced strength is attributed to the mixed composition of carbon, aluminum, and titanium, as well as high-temperature annealing treatment.
It exhibits excellent cold-forming properties, typically associated with nickel-chromium alloys. The grain size results in a pronounced wavy surface texture, known as "orange peel," after multiple cold forming processes. Incoloy 800HT can be welded using standard welding processes.
Both Incoloy 800H and 800HT are commonly used in high-temperature environments exceeding 1100°F (593°C). In corrosive environments and under high-temperature conditions, Incoloy 800H and 800HT are widely used in various fields, including chemical and petrochemical processing, heat treatment equipment, nuclear power plants, and the paper industry.



Gnee Steel offers Incoloy 800/800H/800HT pipe fittings at reasonable prices, customizable to customer needs and based on provided drawings.
Specification Of Incoloy 800/ 800H/ 800HT Pipe Fittings
| Trade name | Incoloy 800 / 800H / 800HT Fittings |
| Specifications : | ASTM B366, B564 / ASME SB366, SB564 |
| Dimensions : | ASTM, ASME and API |
| Standard : | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 / ASME/ANSI B16.9, ASME B16.28, MSS-SP-43 |
| Size Range: | 1/8" NB to 4" NB (Socketweld & Screwed-Threaded) / Seamless 1/2″ – 10″ , Welded 1/2″ – 48″ |
| TYPE | Socketweld Fittings, Screwed-Threaded Fittings / Seamless / Welded / Fabricated |
| Forged Fittings Class | 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS |
| Pipe Fittings Thickness | SCH 5S , 10S ,10, 20 , 40S , 40 , STD , 60 , 80S , 80 , XS , 100 , 120 , 140 , 160 & XXS. |
| Bending Radius | R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom |
| Grade | 800 / 800H / 800HT UNS (N08800, N08810, N08811), DIN (1.4876, 1.4958, 1.4959) |
Incoloy 800/800H/800HT Pipe Fittings Specification
Equivalent Grades of Incoloy 800HT Pipe Fittings
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN | OR |
| Incoloy 800 | 1.4876 | N08800 | NCF 800 | NA 15 | ЭИ670 | Z8NC32-21 | X10NiCrAlTi32-20 | XH32T |
| Incoloy 800H | 1.4958 / 1.4876 | N08810 | NCF 800H | NA 15(H) | ЭИ670 | Z8NC33-21 | X5NiCrAlTi31-20 | XH32T |
| Incoloy 800HT | 1.4859 / 1.4876 | N08811 | NCF 800HT | NA 15(HT) | ЭИ670 | - | X8NiCrAlTi32-21 | XH32T |
Incoloy 800HT Pipe Fittings Chemical Properties
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr | Al | Ti |
|---|---|---|---|---|---|---|---|---|---|---|
| 800 | 0.10 max | 1.50 max | 1.00 max | 0.015 max | 0.75 max | 39.50 min | 30.00 – 35.00 | 19.00 – 23.00 | 0.15 – 0.60 | 0.15 – 0.60 |
| 800H | 0.05 – 0.10 | 1.50 max | 1.00 max | 0.015 max | 0.75 max | 39.50 min | 30.00 – 35.00 | 19.00 – 23.00 | 0.15 – 0.60 | 0.15 – 0.60 |
| 800HT | 0.06 – 0.10 | 1.50 max | 1.00 max | 0.015 max | 0.75 max | 39.50 min | 30.00 – 35.00 | 19.00 – 23.00 | 0.15 – 0.60ᴬ | 0.15 – 0.60ᴬ |
Incoloy 800HT Pipe Fittings Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|---|
| 800 / 800H / 800HT | 7.94 g/cm3 | 1385 °C (2525 °F) | Psi – 75,000 , MPa – 520 | Psi – 30,000 , MPa – 205 | 30 % |
Pressure Rating Of Inconel 800/ 800H/ 800HT Buttweld Fittings
| (oF) | (oC) | 150 |
| -20 to 150 | -29 to 66 | 300 |
| 200 | 93 | 265 |
| 250 | 121 | 225 |
| 300 | 149 | 185 |
| 350 | 177 | 150 |
| 400 | 204 | - |
| 450 | 232 | - |
| 500 | 260 | - |
| 550 | 288 | - |
Incoloy 800/800H/800HT Pipe Fittings Dimension Data Sheet
Manufacturing process of Type 800 Incoloy alloy pipe fittings

Manufacturing process of Type 800 Incoloy alloy pipe fittings
Incoloy 800/800H/800HT Pipe Fittings stock
Incoloy 800HT Elbow
We supply ASTM B366 Incoloy 800 alloy elbows, ASME SB366 Incoloy 800H 90-degree elbows, UNS N08800 and N08810 45-degree elbows, 1.4859 / 1.4876 180-degree weld elbows, and are an exporter of nickel alloy 800HT seamless pipe elbows. We also supply ANSI B16.9 Incoloy 800 weld elbows and are a Chinese manufacturer of Incoloy 800HT weld elbows.


Incoloy 800/800H/800HT Tee
Suppliers of ASTM B366 Incoloy 800 alloy tees, UNS N08800, N08810 equal tees, 1.4859 / 1.4876 reducing tees, ASME SB366 Incoloy 800H reducing tees, ANSI B16.9 Incoloy 800HT pipe tees, exporters of nickel alloy 800 seamless tees, Incoloy 800H weld neck tees, and manufacturers of Incoloy 800HT weld neck tees.
Incoloy 800 Cross
There are locations in the United states of america as well as ationally. The organization was established in 2000 on the basis of a small idea conceived by its promoters that was incepted.


Incoloy 800H/800HT Reducer
Suppliers of ASTM B366 Incoloy 800 alloy reducers, UNS N08800 and N08810 eccentric reducers, 1.4859/1.4876 concentric reducers, ASME SB366 Incoloy 800H eccentric reducers, ANSI B16.9 Incoloy 800HT concentric reducers, exporters of seamless nickel alloy 800 reducers, Incoloy 800H butt-welded reducers, and Incoloy 800HT welded reducers.
Incoloy 800 Pipe Cap
Suppliers of ASTM B366 Incoloy 800 pipe caps, UNS N08800 and N08810 end caps, 1.4859/1.4876 pipe caps, ASME SB366 Incoloy 800H pipe caps, ANSI B16.9 Incoloy 800HT pipe caps, exporters of seamless nickel alloy 800 pipe caps, Incoloy 800H butt-welded pipe caps, and manufacturers of Incoloy 800HT welded pipe caps.


Incoloy Alloy 800H Stub End
Suppliers of ASTM B366 Incoloy 800 alloy short tubes, UNS N08800 and N08810 long and short tubes, 1.4859 / 1.4876 short tubes, ASME SB366 Incoloy 800H long and short tubes, ANSI B16.9 Incoloy 800HT short tubes, exporters of seamless nickel alloy 800 short tubes, Incoloy 800H butt-welded short tubes, and manufacturers of Incoloy 800HT welded short tubes.
Alloy 800HT Pipe Bend
Suppliers of ASTM B366 Incoloy 800 alloy bends, UNS N08800 and N08810 long radius bends, 1.4859/1.4876 short radius bends, ASME SB366 Incoloy 800H U-bends, ANSI B16.9 Incoloy 800HT cleanable bends, exporters of seamless nickel alloy 800 bends, Incoloy 800H butt-welded bends, and Incoloy 800HT welded bends.

Price Of Inconel 800/ 800H/ 800HT Buttweld Fittings
| High Nickel 800 Alloys Elbow | USD $8.11 - $20.21 / Piece (FOB Price) on request |
| High Nickel 800H Alloys Equal Tee | USD $8.11 - $20.21 / Piece (FOB Price) on request |
| High Nickel 800H/800HT Alloys Reducing Tee | USD $8.11 - $20.21 / Piece (FOB Price) on request |
| High Nickel 800HT Alloys Cross | USD $8.11 - $20.21 / Piece (FOB Price) on request |
| High Nickel 800 Alloys Cap | USD $8.11 - $20.21 / Piece (FOB Price) on request |
Incoloy 800 / 800HT / 800HT Pipe Fittings Application
Gnee Steel ensures that all products are made from high-quality raw materials. We conduct rigorous testing on every product before shipping it to our customers.
Petrochemical Industry
Power Generation Industry
Food Processing Industry
Oil & Gas Industry
Sugar Industry


Testing Of Inconel 800/ 800H/ 800HT Buttweld Fittings
Gnee Steel is renowned for its precise dimensions. All products undergo comprehensive testing before shipment. We perform destructive and non-destructive testing on all products.
Eddy current testing
Hydraulic pressure analysis
Pitting corrosion protection testing
Power generation industry
Materials certification
Packing Of Incoloy 800/ 800H/ 800HT Pipe Fitting
Gnee Steel employs the safest and most efficient packaging methods suitable for all types of cargo transportation. Our packaging options are diverse, including:
Wooden Crates
Wooden Pallets
Shrink Film Packaging
Cartons
Wooden Crates

About Gnee Steel

Request the latest price list for INCOLOY 800/800H/800HT pipe fittings. Please call +8615824687445 or email ss@gneesteel.com for information on available stock and the latest price list for INCOLOY 800/800H/800HT, 1.4876/1.4958/1.4859 butt weld fittings.
FAQ
Q: What are INCOLOY 800/800H/800HT butt-welded pipe fittings?
A: Incoloy 800/800H/800HT butt-welded pipe fittings are high-temperature alloy fittings used in industrial applications. They are composed of INCOLOY 800, 800H, and 800HT alloys, all of which are nickel-iron-chromium alloys renowned for their excellent strength and corrosion resistance.
Q: What are the product specifications for INCOLOY 800/800H/800HT butt-welded pipe fittings?
A: Incoloy 800/800H/800HT butt-welded pipe fittings are silver in color and are composed of materials such as carbon steel, stainless steel, nickel, titanium, low-carbon steel, and aluminum. They conform to multiple standards, including AISI, ANSI, ASME, ASTM, DIN, and JIS.
Q: What are the advantages of using INCOLOY 800/800H/800HT fittings?
A: Incoloy 800/800H/800HT fittings have extremely high corrosion resistance, making them ideal for use in high-temperature and corrosive environments. They are also robust and durable, suitable for a wide range of industrial applications.
Hot Tags: incoloy 800/800h/800ht pipe fitting, China incoloy 800/800h/800ht pipe fitting suppliers, incoloy steel tubing, alloy for biofabrication baths, alloy ss tube, incoloy pipe steel, alloy for distillation baths, alloy for crystallization baths