Feb 02, 2026 Leave a message

800/800H/800HT alloy pipe fittings tolerances

800/800H/800HT alloy pipe fittings, tolerances for butt welded pipe fittings, tolerance table for 800 pipe fittings (mm), dimensions of Incoloy 800 butt welded straight-through tee.

 

800/800H/800HT Alloy Pipe Fittings Dimension Table

All Fittings 90, 45 Elbows and Tees Reducers Caps 180 Returns Angularity Tolerance
Nominal Pipe Size Outside Diameter at Bevel Inside Diameter at End Wall Thickness Center to End Dimension Overall Length Overall Length Center to Center Dimension Back to face Dimension Alignment of Ends Nominal Pipe Size off Angle off Plane
(in) D   t A.B.C.M H E O K U (in) Q P
1/2to 21/2 +1.52-0.76 0.76 Not Less Than 87.5% of Nominal Thickness 1.52 1.52 3.05 6.35 6.35 0.76 1/2 to 4 0.76 1.51
3 to 31/2 1.52 1.52 1.52 1.52 3.05 6.35 6.35 0.75 5 to 8 1.52 3.05
4 1.52 1.52 1.52 1.52 3.05 6.35 6.36 0.76 10 to 12 2.29 4.83
5 to 8 +2.29-1.52 1.52 1.52 1.52 6.35 6.35 6.35 0.76 14 to 16 2.29 6.35
10 to 18 +4.06-3.05 3.05 2.29 2.29 6.35 9.65 6.35 1.52 18 to 24 3.05 9.65
20 to 24 +6.35-4.83 4.83 2.29 2.29 6.35 9.65 6.35 1.52 26 to 30 4.83 9.65
26 to 30 +6.35-4.83 4.83 3.05 4.83 9.65 – – – 32 to 36 4.83 12.7
32 to 36 +6.35-4.83 4.83 4.83 4.83 9.65 – – –      

Send Inquiry

whatsapp

Phone

E-mail