864 903 Metal Seamless Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 864 903 metal seamless pipe in China. If you're going to wholesale high quality 864 903 metal seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
incoloy Products Application
incoloy 864 903 Metal Seamless Pipe video
Incoloy 903 alloy has excellent corrosion resistance and fatigue resistance. It has a longer fatigue life than steel and other alloys under repeated loading. Incoloy 903 alloy can maintain its excellent performance for a long time under the harsh conditions of high temperature, high flight, and high load, making it an ideal material for the aerospace, automotive, petroleum, and energy industries. In the aerospace field, aircraft engines need to withstand high temperature, high load, and high stress environments, so the requirements for materials are very high. As a high-temperature alloy with excellent fatigue resistance, Incoloy 903 alloy can maintain its strength and stability at high temperatures, thus ensuring the safety and reliability of aircraft.
incoloy Material Specification
| Element | Content (%) |
|---|---|
| Nickel, Ni | 30 – 38 |
| Iron, Fe | 29.105 – 45 |
| Chromium, Cr | 20 – 25 |
| Molybdenum, Mo | 4 – 4.8 |
| Silicon, Si | 0.60 – 1 |
| Titanium, Ti | 0.40 – 1 |
| Carbon, C | ≤ 0.080 |
| Sulfur, S | ≤ 0.015 |


GH4648 superalloy is a Ni-Cr-based precipitation hardening deformed superalloy. The long-term use temperature is less than 900°C, and the short-term use temperature can reach 1100°C. The alloy is characterized by the addition of approximately 32% ω (Cr), which gives it excellent resistance to hot corrosion. At the same time, the alloy has medium strength, good fatigue and creep resistance, good cold working performance and welding performance. It is suitable for making high-temperature structural parts with temperatures between 900℃~1100℃ and requiring excellent corrosion resistance. The main varieties supplied are plates, strips, pipes, bars, forgings and rings.
Low-expansion high-temperature alloy Incoloy 903 is a Ni-Fe-Co-based alloy reinforced with Nb. Ti and A1 elements. Its outstanding features are low thermal expansion coefficient, almost constant elastic modulus, high temperature and excellent thermal fatigue resistance. performance, and the ability to resist embrittlement in high-pressure hydrogen environments. Therefore, the alloy is widely used in parts of aircraft engine compressors, turbines and space shuttle main rocket engines.
Customer Case
customer visit


FAQ
Q: Are you a factory or a trading company?
A: We are a professional manufacturer, and our company is also a very professional steel products trading company. We can offer a wide range of steel as well as super stainless steel products.
Q: What does your factory do in terms of quality control?
A: We have obtained ISO, CE and other certifications. From materials to products, we check every process to maintain good quality.
Q: Can I get a sample before ordering?
Answer: Yes, of course. Usually our samples are free. We can produce according to your samples or technical drawings.
Q: About the product price of 864 903 Metal Seamless Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Hot Tags: 864 903 metal seamless pipe, China 864 903 metal seamless pipe suppliers, alloy for 3d printing baths, alloy for transformers, alloy for oxidation resistance, alloy for gasket materials, alloy for flexible manufacturing baths, alloy for electron beam melting baths
You Might Also Like
Send Inquiry