GH3536 3230 High Temperature Alloys Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh3536 3230 high temperature alloys pipe in China. If you're going to wholesale high quality gh3536 3230 high temperature alloys pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
GH3536 3230 High Temperature Alloys Pipe
Density:8.44 g/c㎡
Melting range:1290-1350℃
Size: OD 25~320mm
W.T: 0.5 - 100mm
Length: 5.8m, 6m, 11.8m, 12m
Type: Seamless/welded
Standards:
Seamless Pipe / Tube: ASTM B444, ASTM B829, AMS 5581
Welded Pipe/tube: ASTM B705, ASTM B775, ASTM B704, ASTM B751
GH3230, a Ni-Cr-based solid solution strengthened deformed superalloy, has attracted much attention for its excellent performance over a wide temperature range (700-1050 degrees Celsius). This alloy not only has excellent high-temperature strength and thermal fatigue resistance, but also maintains excellent structural stability. GH3230 material is widely used in the manufacture of high-temperature parts such as aircraft engine barrels due to its excellent hot corrosion resistance.
Features of GH3230 material:
GH3230 superalloy exhibits excellent high-temperature strength and excellent resistance to thermal and cold fatigue. The alloy's structure remains stable, allowing it to perform well in extreme environments. In addition, the alloy also has excellent hot corrosion resistance and is suitable for long-term use in high temperature and corrosive environments.
Ingredient content of GH3230 material:
Carbon C: 0.5-0.15
Silicon Si: 0.25-0.75
ManganeseMn: 0.3-1.0
Phosphorus P: ≤0.03
Sulfur S: ≤0.015
Chromium Cr: 20-24
Nickel Ni: Yu
Molybdenum: 1-3
Lanthanum La: 0.005-0.05
CopperCu: ≤0.50
Iron: ≤3.00
NiobiumNb: ~
Boron B: ≤0.015
Titanium Ti: ≤0.10
Aluminum Al: 0.2-0.5
Vanadium V: ~
Tungsten W: 13-15
Cerium Ce: ~