N S Hastelloy Metal Pipe
video

N S Hastelloy Metal Pipe

Hastelloy N alloy is a nickel-based high-temperature alloy material used in molten salt reactors. It has excellent corrosion resistance, resistance to neutron radiation and good high-temperature mechanical properties.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of n s hastelloy metal pipe in China. If you're going to wholesale high quality n s hastelloy metal pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

N S Hastelloy Metal Pipe

GNEE STEEL COMPANY

Our company is engaged in the production and trade of various N S Hastelloy Metal Pipe, high-performance, high-precision special-shaped steel pipes and seamless pipes. We have established business relationships with customers in more than 20 countries and regions. Details such as payment method, delivery time and minimum quantity can be negotiated based on the order.

 

Hastelloy N is used in chemical process equipment and general industrial applications where high temperature oxidation resistance is required.
aerospace
transportation
consumer
defense
industrial

N S Hastelloy Metal Pipe Specification

 

Element Content (%)
Nickel, Ni 71
Molybdenum, Mo 16
Chromium, Cr 7
Iron, Fe ≤ 5
Silicon, Si ≤ 1
Manganese, Mn ≤ 0.80
Tungsten, W ≤ 0.50
Aluminum, Al + Titanium, Ti ≤ 0.50
Copper, Cu ≤ 0.35
Cobalt, Co ≤ 0.20

N S Hastelloy Metal Pipe

N S Hastelloy Metal PipeN S Hastelloy Metal Pipe

Hot Tags: n s hastelloy metal pipe, China n s hastelloy metal pipe suppliers, alloy for electrochemical applications, alloy for quenching, alloy for distillation columns, seamless ss pipe, alloy for fuel cells, hastelloy alloy piping