UNS N06059 X Hastelloy Metal Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns n06059 x hastelloy metal pipe in China. If you're going to wholesale high quality uns n06059 x hastelloy metal pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
UNS N06059 X Hastelloy Metal Pipe
GNEE STEEL COMPANY
Our company is engaged in the production and trade of various UNS N06059 X Hastelloy Metal Pipe, high-performance, high-precision special-shaped steel pipes and seamless pipes. We have established business relationships with customers in more than 20 countries and regions. Details such as payment method, delivery time and minimum quantity can be negotiated based on the order.
Application overview and special requirements of Hastelloy X (N06002): This alloy has been widely used in foreign aerospace engines and civil industries. Our country is mainly used to manufacture combustion chamber parts and other hot-end parts and honeycomb structural parts. . This alloy has a certain age hardening phenomenon after long-term use at high temperatures.
gas turbine
Petrochemical industry
industrial furnace
Heat treatment equipment
nuclear engineering
jet engine combustion chamber
aircraft cabin heater
turbine exhaust components
UNS N06059 X Hastelloy Metal Pipe Specification
| Properties | Metric | Imperial |
|---|---|---|
| Tensile strength (@sheet and strip 0.5 to 6.4 mm) | 690 MPa | 100000 psi |
| Yield strength (@rod, bar, forgings > 100 mm) | 320 MPa | 46400 psi |
| Modulus of elasticity | 210 GPa | 30500 ksi |
| Elongation at break | 40% | 40% |
UNS N06059 X Hastelloy Metal Pipe


Hot Tags: uns n06059 x hastelloy metal pipe, China uns n06059 x hastelloy metal pipe suppliers, alloy for catalytic converters, alloy for furnaces, UNS N06455 N10629 Hastelloy Pipe, alloy for annealing, NI MO corrosion alloy, seamless ss pipe