Hastelloy G30 Round Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy g30 round bar in China. If you're going to wholesale high quality hastelloy g30 round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hastelloy G30 Round Bar
Product Introduction
Hastelloy G-30 is a high performance nickel alloy. Its chemical composition is carefully controlled to provide excellent corrosion resistance and high temperature performance. Through precise manufacturing processes and high quality material selection, our Hastelloy G-30 round bars and rods have excellent properties such as high strength, corrosion resistance, oxidation resistance and creep resistance. These properties make our round bars widely used in chemical, petroleum, pharmaceutical, aerospace and other fields.
| Product name | G30 Hastelloy bar |
|
Specifications |
ASTM B574 / ASME SB574 |
|
Grade |
G30 Hastelloy – UNS N06030 |
|
Diameter |
5 mm To 500 mm |
|
Length |
100 mm To 3000 mm Long & Above |
|
Finish |
Bright, Polish & Black |
|
Form |
Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc. |
|
Tolerance |
H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients' requirements |
Equivalent Grades
| Grade | UNS | Werkstoff Nr. |
| Hastelloy G-30 | DIN 2.4603 | UNS N06030 |
Chemical Composition
| Ni | Cr | Fe | Mo | Cu | Mn | Co | C | W | Si | P | S | Nb+Ta |
| Rem | 28.0-31.5 | 13.0-17.0 | 4.0-6.0 | 1.0-2.4 | 1.5 | 5.0 | 0.03 | 1.5-4.0 | 0.8 | 0.04 | 0.02 | 0.30-1.50 |
Mechanical Properties
| Tensile Strength, Min ksi | Yield Strength, (0.2% offset), Min, ksi | Min. Elongation in 2″, % | Density lb/in³ |
| 85 | 35 | 30.0 | 0.297 |
Hot Tags: hastelloy g30 round bar, China hastelloy g30 round bar suppliers, alloy for valves, alloy for grinding, Hastelloy Alloy C22 Round Bars, alloy for welding, alloy for pumps, alloy for compressors