Hastelloy C22 hot rolled Seamless Alloy Pipe
Sizes: 1/2" OD - 12" OD
OD: 3.00mm - 219.10mm
Thickness: 0.40mm - 12.70mm
Lengths: Single Length, Double Length, Random Length and Cut Length
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy c22 hot rolled seamless alloy pipe in China. If you're going to wholesale high quality hastelloy c22 hot rolled seamless alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hastelloy C22 hot rolled ss Alloy Pipe introduce
Hastelloy C22 hot rolled Seamless Pipe


Hastelloy C22 seamless pipe is having the strong soldering capacity. It is because the consumed filler wires and electrodes have high corrosion resistances. The same smooth bore Hastelloy C22 pipes are the best for bleaching, brackish water, enclosed water systems and certain other maritime conditions. Nickel alloys are used to counter the sour gas and oil fields, the ones that opt for this incredible performance.
Hastelloy C22 Pipes Specification
| Standard | ASTM B 622, B 619 / ASME SB 622, SB 619 |
| Standard | ASTM, ASME and API |
| Size | 15 NB UP TO C22 NB IN SCH 5S, 10S,10, 20, 40S, 40, STD, 60, 80S, 80, XS, 100, 120, 140, 160 & XXS |
| Length | Single Random, Double Random & Required Length, Cut Length |
| End | Plain End, Beveled End, Treaded |
Hastelloy C22 Pipes Chemical Properties
| Grade | C | Mn | Si | Co | P | Fe | Mo | Ni | Cr | S | W | V |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Hastelloy C22 | 0.010 max | 0.50 max | 0.08 max | 2.5 max | 0.02 max | 2 – 6 | 12.5 – 14.5 | Bal | 20 – 22.5 | 0.02 max | 2.5 – 3.5 | 0.35 max |
GNEE Group Factory Environment
Hastelloy C22 hot rolled ss Pipe

GNEE Group Product Packaging
C22 hot rolled ss Alloy Pipe

FAQ
Q: How do you control quality ?
A: Mill test certification is supplied with shipment, third party inspection is available. And we also get ISO, SGS, Alibaba Verified.
Q: How many coutries you already exported ?
A: We have become trade partners with more than 50 countries around the world, mainly exporting to the United States, Britain, Kuwait, Egypt, Türkiye, Jordan, India, etc.
Q: Can you provide sample ?
A: Of course! As long as you contact us, we can provide free inventory samples. Customized samples take approximately 5-10 days.
Hot Tags: Hastelloy C22 hot rolled Seamless Alloy Pipe, China Hastelloy C22 hot rolled Seamless Alloy Pipe suppliers, stainless steel pipe, alloy for coating, alloy for compressors, Hastelloy C, hastelloy material piping alloy, alloy for drawing