Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of haselloy uns n10665 alloy pipe in China. If you're going to wholesale high quality haselloy uns n10665 alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Haselloy UNS N10665 Alloy Pipe
It is widely used in chemical, petrochemical, power generation and pollution control fields, especially in sulfur, hydrochloric acid, phosphorus, acetic acid and other industries. If used in special areas, please contact the material supplier.
Haynes556 (UNS R30556) alloy is an iron-nickel-chromium-cobalt alloy that effectively resists vulcanization, carburization and chlorine atom environments at high temperatures, and has good oxidation resistance and excellent high-temperature strength. It has also been found to be resistant to corrosion from molten salts and other salts, and to corrosion from molten zinc.
welding
Welding of HAYNES 556 alloy is performed by commonly used welding techniques such as gas tungsten arc welding, shielded metal arc welding, metal arc welding and submerged arc welding. However, an alloy filler metal suitable for this alloy should be used.
characteristic:
UNS R30556 combines the properties of resistance to vulcanization, carburization and corrosion in chlorine-containing media under high temperature environments, anti-oxidation, easy processing and excellent high-temperature strength. It has corrosion resistance to molten zinc, molten chloride salts and other salts.
application:
Industrial waste incinerators, rotary calciners, hot-dip galvanizing equipment and high-temperature components for the aerospace industry.