Hastelloy C-2000 Raw Materials Alloy Sheet
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy c-2000 raw materials alloy sheet in China. If you're going to wholesale high quality hastelloy c-2000 raw materials alloy sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hastelloy C-2000 Raw Materials Alloy Sheet
Physical Properties
Density:8.9 g/cm3, Melting Point:1325-1370 ºC
Mechanical Properties of Alloys at Room Temperature Min
1,Hastelloy C22(N06022)Tensile strength of nickel-based alloys Rm N/mm2:690
2,Hastelloy C22(N06022)Yield strength of nickel base alloy RP0.2N/mm2:283
3,Hastelloy C22(N06022)Elongation of nickel base alloy A5 %:40
Corrosion Resistance of Alloys
1)Hastelloy C22 alloys are suitable for a variety of chemical process industries containing oxidizing and reducing media.
2) The high content of molybdenum and chromium makes the alloy resistant to chloride ions, and tungsten further improves its corrosion resistance.
3)Hastelloy C22 is one of the only materials capable of resisting the corrosion of moist chlorine, hypochlorite and chlorine dioxide solutions.
4)The alloy has excellent corrosion resistance to high concentrations of salt chloride solutions (such as ferric chloride and copper chloride).