654SMO Super Duplex Stainless Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 654smo super duplex stainless pipe in China. If you're going to wholesale high quality 654smo super duplex stainless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
654SMO Super Duplex Stainless Pipe
GNEE STEEL COMPANY
Our company is engaged in the production and trade of various 654SMO UNS S31727 Super Duplex Stainless Tube, high-performance, high-precision special-shaped steel pipes and seamless pipes. We have established business relationships with customers in more than 20 countries and regions. Details such as payment method, delivery time and minimum quantity can be negotiated based on the order.
C:≤0.02
Si:≤0.05
Mn:2.00-4.00
Ni:21.0-23.0
P:≤0.03
S:≤0.005
Cr:23-25
Mo:7.0-8.0
N:0.45 - 0.55
Cu:0.3-0.6
Hot Tags: 654smo super duplex stainless pipe, China 654smo super duplex stainless pipe suppliers, 2 4668 Nickel Alloy Steel Coil, Uns N06600 Alloy tubing, Ni36CrTiAl Plate, Hastelloy C 22 Alloy Steel Flange, Monel 400 Alloy Steel Sheet, Alloy Steel 600 plate