Hastelloy B2 Corrosion resistant Steel Sheet
Size: 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm
Thickness: 0.1mm to 100 mm
Width: 10-2500mm
Length: 2m, 2.44m, 3m or customized as required
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy b2 corrosion resistant steel sheet in China. If you're going to wholesale high quality hastelloy b2 corrosion resistant steel sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hastelloy B2 Steel Sheet introduce
Hastelloy B2 Corrosion resistant Sheet


Hastelloy B2 Sheet is a base of nickel developed with excellent resistance and all concentrations to hydrochloric acids. It is ideal for the reduction of chlorides, sulfides and alkalis. The material of molybdenum is a central component of alloy. It can be used in the conditions as soldered. Such sheets and plates endure horrible production and handling conditions.
Hastelloy B2 Sheet has good working ability that can be molded according to their use. Having the workmanship of these sheets and plates is also a good feature. They are also good soiling.
Hastelloy B2 Sheet & Plate Specification :
| Specifications | : | ASTM B333 / ASME SB333 |
|---|---|---|
| Dimensions | : | ASTM, ASME, and API |
| Thickness | : | Ranging from 0.3mm to 20mm |
| Length | : | 2000 mm / 2440 mm / 2500 mm / 3000 mm / 6000 mm |
| Hardness | : | As per ASME A & NACE MR 175 |
| Width | : |
1000mm / 1219mm /1250mm / 1500mm / 2000mm |
| Finish | : | Hot rolled plate (HR), Cold rolled sheet (CR) |
| Form | : | Coils, Foils, Rolls, Plain Sheet, Strip, Flats, Blank (Circle), Ring (Flange) etc. |
Chemical Composition of Hastelloy B2 Sheets and Plates
| Grade | C | Mn | Si | S | Co | Ni | Cr | Fe | Mo | P |
| Hastelloy B2 | 0.02 max | 1.0 max | 0.1 max | 0.03 max | 1.0 max | Bal | 1.0 max | 2.0 max | 26 – 30 | 0.04 max |
GNEE Group Factory Environment
B2 Corrosion resistant Steel Sheet

GNEE Group Product Packaging
metal B2 Corrosion resistant Steel Sheet

GNEE Group Product Testing
alloy B2 Corrosion resistant Steel Sheet

FAQ
Q: What is your terms of payment?
A: 20% Prepayment and balance see B/L copy or 100%LC at sight.
Q: Are you a factory or a trading company?
A: We are a professional manufacturer, and our company is also a very professional steel products trading company. We can offer a wide range of steel as well as super stainless steel products.
Q: What does your factory do in terms of quality control?
A: We have obtained ISO, CE and other certifications. From materials to products, we check every process to maintain good quality.
Hot Tags: Hastelloy B2 Corrosion resistant Steel Sheet, China Hastelloy B2 Corrosion resistant Steel Sheet suppliers, alloy for boilers, alloy for electrochemical applications, alloy for surface treatment, alloy for pumps, material seamless piping, stainless steel pipe
You Might Also Like
Send Inquiry