C22 G3 Hastelloy Alloy Corrosion Resistant Pipe
video

C22 G3 Hastelloy Alloy Corrosion Resistant Pipe

WNR 2.4602 seamless pipe

Outer diameter: 3-600 mm
Wall thickness: 0.5-30 mm
Length: 0.5-12 m
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of c22 g3 hastelloy alloy corrosion resistant pipe in China. If you're going to wholesale high quality c22 g3 hastelloy alloy corrosion resistant pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

C22 G3 Hastelloy Alloy Pipe Equivalent grade

C22 G3 Hastelloy Alloy Pipe video

GNEE STEEL GROUP supplies C22 G3 Hastelloy Alloy Pipe for you

 

GNEE STEEL GROUP supplies Hastelloy C22 Alloy Pipe

UNS Number N06022

W.Nr. 2.4602

Other common names: Alloy C22

ASTM B574, B564, B575, B619, B626, B622

ASME SB574, SB564, SB575, SB619, SB626, SB622

What forms of Hastelloy C22 does GNEE STEEL offer?
bar
sheet
plate
Pipes and Tubes – Welded and Seamless
Accessories
Elbows, tees, short pipe ends, return pipes, pipe caps, crosses, reducers, pipe joints. ETC.
Welding wire (AWS classification: ERNiCrMo-4 and ENiCrMo-4)

GNEE STEEL GROUP supplies Hastelloy C4 Alloy Pipe

W.NR 2.4610
UNS N06455
AWS 052

 

GNEE STEEL GROUP supplies G3 Hastelloy Alloy Pipe

ASTM Specifications

Pipe Smls Pipe Welded Tube Smls Tube Welded Sheet / Plate Bar Forging Fitting

B622

B619

B622

B626

B333

B335

B564

B366

GNEE STEEL GROUP supplies Hastelloy G-3 tube

 

Hastelloy G-3 Forms
We can provide Hastelloy G-3 in various forms according to your customization, such as:

Hastelloy G-3 Bar Hastelloy G-3 Sheet&Plate
Hastelloy G-3 Welded Pipe&Tube Hastelloy G-3 Seamless Pipe&Tube
Hastelloy G-3 Pipe Fittings Hastelloy G-3 Fasteners
Hastelloy G-3 Forgings Hastelloy G-3 Flanges
Hastelloy G-3 Coil Hastelloy G-3 wire

 

C22 G3 Hastelloy Alloy Pipe chemical composition

C22 Hastelloy Alloy Pipe chemical composition

Chemical Requirements

 

Ni

Cr

Mn

C

Mo

Si

Fe

Max

Bal.

22.5

0.50

0.015

14.5

0.08

6.0

Min

 

20.0

 

 

12.5

 

2.0

G3 Hastelloy Alloy Pipe chemical composition

The Chemical Composition of Hastelloy G3 %
Ni Balance
Co ≤5.0
Cr 28.0-31.5
Mo 4.0-6.0
W 1.5-4.0
Fe 13.0-17.0
Si ≤0.8
Mn ≤1.5
C ≤0.03
Cb+Ta 0.3-1.5
Cu 1.0-2.4
P ≤0.04
S ≤0.02

C22 G3 Hastelloy Alloy Pipe

C22 G3 Hastelloy alloy Piping suppliersC22 G3 Hastelloy steel tube dealer

Hastelloy C-22 alloy is an all-around nickel-chromium-molybdenum-tungsten alloy that has better overall corrosion resistance than other nickel-chromium-molybdenum alloys (including Hastelloy C-276, C4 and Inconel 625). Hastelloy C-22 alloy has good resistance to pitting corrosion, crevice corrosion and stress corrosion cracking.
Hastelloy G3 has excellent resistance to oxidation, atmospheric corrosion and stress corrosion cracking, and has high resistance to local corrosion (pitting corrosion, crevice corrosion). Due to the high Fe content in the alloy, it has the characteristics of low cost compared with other nickel-based corrosion-resistant alloys. G3 alloy is commonly used in flue gas desulfurization systems, papermaking, and phosphoric acid production steam generators and heat exchangers.

GNEE Group Factory Environment

C22 G3 Alloy Corrosion Resistant Pipe

C22 G3 Hastelloy Alloy Corrosion Resistant Pipe

C22 G3 Hastelloy Alloy Pipe material & size

C22 G3 Hastelloy Alloy Pipe material & size

C22 G3 Hastelloy Alloy Pipe

C22 G3 Hastelloy Alloy Pipe

 

Customer Case

customer visit

C22 G3 Hastelloy Alloy Pipe

 

AQ

Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.

Q: What shipping ports are there?
A: Generally, we ship from Tianjin Port, you can choose other ports according to your needs.

Q: About the product price?
Answer: Due to cyclical changes in raw material prices, prices vary in different periods.

Q: About the product price of C22 G3 Hastelloy alloy Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Contact Us

 

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

 

Hot Tags: C22 G3 Hastelloy Alloy Corrosion Resistant Pipe, China C22 G3 Hastelloy Alloy Corrosion Resistant Pipe suppliers, alloy for drawing, alloy for grinding, hastelloy metal pipe, Hastelloy Alloy C22 Round Bars, alloy for cold working, alloy for finishing

Send Inquiry

whatsapp

Phone

E-mail

Inquiry