Duplex is a powerful austenitic and ferritic dual-microstructure grade. The duplex plate has a chemical composition of carbon, manganese, silicon, phosphorous, sulfur, chromium, molybdenum, nickel, nitrogen, and copper. Duplex stainless steel plate has excellent corrosion resistance and tolerance in harsh environments. The plates are tolerant to crevice corrosion and pitting by chlorides. The s2205 is a common grade of the duplex grade. The duplex plate supplier subject the plates to harsh conditions and has a temperature limit below 600 degrees f. These plates can be easily welded following standard procedures.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns s32760 plate in China. If you're going to wholesale high quality uns s32760 plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

The plates contain chromium nickel and molybdenum in highest quantities and rest are copper, tungsten and nitrogen in small amounts. UNS S32760 plate is also specified as super duplex stainless steel plate which is highly reliable and resistant to corrosion. The plates display absolute toughness and excellent smooth surface finishing. S32760 plate are extensively used in variety of industrial applications such as seawater systems, subsea pipework systems, desalination plants, centrifuges, flue gas desulphurisation (FGD), construction, pressure vessels, valve and pumps. These plates are capable of handling heavy loads, high pressure and stress. UNS S32760 sheet are highly durable and be used in various high temperature and pressure applications.

S32760 steel cold rolled plate display excellent resistance against sulphide-stress corrosion cracking is sour gas conditions. This material is very popular for its high impact strength. UNS S32760 hot rolled plate are strongly designed with smooth surface finish with no blunt edges providing ease in installation and maintenance of the material. The plates are strongly designed with excellent thermal conductivity properties.

The plates exhibit excellent heat tolerance capacity and can be used in wide range of high temperature applications with strong melting of 13500C. The density of these plates is 7810kg/m3 with strong yield strength of 550 MPa. The delivery conditions of the plates include rolled, annealed, water quenched and oil quenched.

321 Stainless Steel Medium Thick Plate321 Stainless Steel Medium Thick Plate

product-369-360product-800-800

FAQ

Q: How long is your delivery time?

A: It is according to quantity. Generally it is 30 days.

Q: Can you provide us sample, is it free or need to pay?

A: If you don't need to print your logo or other artwork on the products, we will not charge any cost, just tell us your freight collect account like Fedex, DHL, TNT. If you don't have, we need to charge Express fee properly.

Q:What are the shipping ports?

A:Under normal circumstances, we ship from Shanghai, Tianjin, Qingdao, Ningbo ports, you can choose other ports according to your needs.

Q:About product prices?

A:Prices vary from period to period due to cyclical changes in the price of raw materials.

Hot Tags: uns s32760 plate, China uns s32760 plate suppliers, duplex stainless steel producer, duplex stainless steel newsletter, duplex stainless steel user, duplex stainless steel vessel, duplex stainless steel acid resistance, duplex stainless steel performance

Send Inquiry

whatsapp

Phone

E-mail

Inquiry