Duplex Stainless Steel 2202 Plate
video

Duplex Stainless Steel 2202 Plate

Duplex 2205: Duplex 2205 is the most widely used duplex stainless steel. It contains 22% chromium, 5% nickel, and 3% molybdenum. It has high strength, excellent corrosion resistance, and is often used in chemical processing, oil and gas, and marine applications.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of duplex stainless steel 2202 plate in China. If you're going to wholesale high quality duplex stainless steel 2202 plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Products Description

Duplex Steel 2202 Plate

2202 duplex stainless steel sheet is a cost effective solution for many applications where the 300 series stainless steels are susceptible to chloride stress corrosion cracking. Stress corrosion cracking occurs when stainless steels are subjected to tensile stress, while in contact with solutions containing chlorides. Increasing temperatures also increase the susceptibility of stainless steels to stress corrosion cracking.

The combination of chromium, molybdenum and nitrogen convey the good resistance of 2202 to chloride pitting and crevice corrosion. This resistance is extremely important for services such as marine environments, brackish water, bleaching operations, closed loop water systems and some food processing applications. The high chromium, molybdenum and nitrogen contents of 2202 provide corrosion resistance superior to common stainless steels, such as, 316L and 317L in most environments.

 

Products Properties


Chemical Composition

Grade

 

C

Mn

Si

P

S

Cr

Mo

Ni

N

2202

Min

Max

-

0.030

-

2.00

-

1.00

-

0.030

-

0.020

21.0

23.0

2.5

3.5

4.5

6.5

0.08

0.20


Mechanical Properties

Grade

Tensile Str
(MPa) min

Yield Strength
0.2% Proof
(MPa) min

Elongation
(% in 50mm) min

Hardness

Rockwell C (HR C)

Brinell (HB)

2202

621

448

25

31 max

293 max

 

Duplex Stainless Steel 2202 Plate

Duplex Stainless Steel Sheet

Duplex steel sheets of 2202 are a cost-effective solution for a number of applications where chloride stress corrosion cracking is subject to the 300 series of stainless steels. Stress corrosion cracking occurs when tensile stresses on stainless steels while they are in contact with chloride solutions. Increasing temperatures also increase the susceptibility to stress cracking of stainless steels. The chromium, molybdenum and nitrogen combination convey the good chloride resistance and corrosion rates of 2202. In most environments, the high content of 2202 chromium, molybdenum and nitrogen gives superior resistance to corrosion to common stainless steels, for instance 316L and 317L.Resistance is important in Services such as marine environments, brackish water, bleaching, closed loop water systems and certain food processing applications.

 

Duplex plate 2202, or plate DX2202, is an austenitic-ferritic stainless steel. It offers users general corrosion resistance comparable to that of Type 304L . Some of the other key characteristics of Duplex 2202 include:

  • Improved mechanical strength
  • Service temperature range of -50 °C to 300°C
  • Stress corrosion resistance that is often double other austenitic stainless steels
  • Can be used in combination with nitric acid

 

Customer Case

 

12405

About US

 

 Rich Experience

GNEE Steel Group was founded in 2008 and has more than 10 years of experience in manufacturing steel.

 

 One-Stop Solution

GNEE Steel Group is a professional, one-stop supply chain enterprise for steel products, covering product research and development, sales, promotion, and providing professional services.

 

 Broad Market

The company's products are sold to Europe, Australia, and exported to more than 70 countries around the world. It has a total of more than 800 global cooperative enterprises, which include 15 shipbuilding companies, 143 engineering project companies, and 23 boiler machinery manufacturers.

 

 Delivery on Time

Our annual product sales volume is 1 million tons, our inventory is 200,000 tons, and our annual export volume has reached 80,000 tons, ensuring on-time delivery.

 

FAQ

 

Q: What are your payment terms?
A:30% T/T in advance, 70% balance before shipment or based on copy of bill of lading or L/C at sight.
Q: What about product pricing information?
A:Prices vary due to regular changes in raw material prices.
Q: Can I send samples?
A:Of course, we provide free samples and express delivery to customers all over the world.
Q: Do you provide customized product services?
A:Yes, we can produce according to your specifications and drawings.
Q: Can I visit your factory?
A:Customers from all over the world are welcome to visit our factory.

Hot Tags: duplex stainless steel 2202 plate, China duplex stainless steel 2202 plate suppliers, duplex stainless steel energy efficiency, duplex stainless steel material, duplex stainless steel hardness, duplex stainless steel use, duplex stainless steel warranty, duplex stainless steel technical data

Send Inquiry

whatsapp

Phone

E-mail

Inquiry