LDX 2101 And 2304 Duplex Stainless Steel Plates
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ldx 2101 and 2304 duplex stainless steel plates in China. If you're going to wholesale high quality ldx 2101 and 2304 duplex stainless steel plates made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
LDX 2101 and 2304 duplex stainless steel plates are high-quality materials that are widely used in various industries. These two types of stainless steel plates offer excellent corrosion resistance, high strength, and good weldability.

LDX 2101 is a low nickel, nitrogen-enhanced duplex stainless steel material that has superior corrosion resistance compared to conventional stainless steels. This material is ideal for applications where high corrosion resistance, high strength, and good weldability are required. LDX 2101 is often used in the chemical, petrochemical, and food processing industries.
On the other hand, 2304 duplex stainless steel offers a high level of corrosion resistance in a wide range of environments. This material is ideal for applications where high strength, excellent toughness, and good weldability are required. Additionally, 2304 duplex stainless steel offers good resistance to stress corrosion cracking and pitting.
| Specification | LDX 2101 | 2304 |
|---|---|---|
| Thickness Range (mm) | 0.5 - 50 | 1 - 50 |
| Width Range (mm) | 1000 - 2500 | 1000 - 2000 |
| Length Range (mm) | 2000 - 12000 | 2000 - 5500 |
| Material Density (g/cm³) | 7.7 | 7.8 |
| Tensile Strength (MPa) | Up to 1000 | Up to 800 |
| Yield Strength (MPa) | Up to 800 | Up to 550 |
| Elongation (%) | 25 - 35 | 25 - 35 |
| Hardness (HRC) | Up to 32 | Up to 30 |
| Corrosion Resistance | Excellent in acidic and chloride-containing environments | Superior in acidic and chloride-containing environments |

Both LDX 2101 and 2304 duplex stainless steel plates are cost-effective solutions that provide excellent performance in various applications. These materials are easy to work with, making them ideal for construction and fabrication projects.
In conclusion, LDX 2101 and 2304 duplex stainless steel plates are excellent materials that offer a wide range of benefits. They are widely used in various industries due to their superior corrosion resistance, high strength, and good weldability. If you are looking for a cost-effective and reliable material for your next project, LDX 2101 and 2304 duplex stainless steel plates are the perfect choice for you.
Hot Tags: ldx 2101 and 2304 duplex stainless steel plates, China ldx 2101 and 2304 duplex stainless steel plates suppliers, duplex stainless steel refund, duplex stainless steel profile, duplex stainless steel rod, duplex stainless steel valve, duplex stainless steel item, duplex stainless steel strength