Alloy LDX 2101 is a lean duplex stainless steel with a balanced composition of chromium, nitrogen, and manganese. It offers a combination of high mechanical strength and good corrosion resistance, making it suitable for various applications.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of duplex alloy ldx 2101 steel plate in China. If you're going to wholesale high quality duplex alloy ldx 2101 steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy LDX 2101 is a lean duplex stainless steel with a balanced composition of chromium, nitrogen, and manganese. It offers a combination of high mechanical strength and good corrosion resistance, making it suitable for various applications.

 

LDX 2101 is a low-nickel, nitrogen enhanced lean duplex stainless steel developed for general-purpose use. The austenitic-ferritic (duplex) structure of the alloy is balanced to approximately equal amounts of ferrite and austenite in the solution-annealed condition.

The high chromium and nitrogen content of LDX 2101, combined with an addition of molybdenum, provide very good resistance to localized and uniform corrosion. The duplex microstructure contributes to the alloys high strength and resistance to chloride stress-corrosion cracking. LDX 2101 possesses both superior strength and greater chloride stress-corrosion cracking resistance than conventional 300 series stainless steels.

4 350

Chemical Analysis

Typical Values (Weight %)

       
Chromium 21.0 min. - 22.0 max. Nickel 1.35 min. - 1.70 max.
Manganese 4.00 min. - 6.00 max. Molybdenum 0.10 min. - 0.80 max.
Nitrogen 0.20 min. - 0.25 max. Chromium 0.040 max.
Silicon 1.00 max. Phosphorus 0.040 max.
Copper 0.10 min. - 0.80 max. Nitrogen 0.030 max.

15

The corrosion resistance of LDX 2101 is generally good making it suitable for use in a wide variety of applications. In most environments, it is superior to 304L stainless steel and comparable to the molybdenum containing 316L stainless steel.

The enhanced mechanical strength of LDX 2101 is far superior to conventional 300 series stainless steels enabling it to be used in thinner cross-sections which can provide significant cost savings to the end user.

LDX 2101 exhibits good abrasion and erosion resistance and can be fabricated using standard shop practices developed for duplex stainless steels.