ASTM B168 Hot Rolled Inconel 601 Stainless Steel Plates
video

ASTM B168 Hot Rolled Inconel 601 Stainless Steel Plates

ASME SB 168 N06600 Sheet

Thickness: 0.1 to 5.0 mm
Width:0.5 to 1.0 meter
Length: 0.7 to 6.0 meter

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b168 hot rolled inconel 601 stainless steel plates in China. If you're going to wholesale high quality astm b168 hot rolled inconel 601 stainless steel plates made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM B168 Inconel 601 Stainless Steel Plates introduce

ASTM B168 Hot Rolled Inconel 601 ss Steel Plates

ASTM B168 Hot Rolled Inconel 601 Stainless Steel PlatesASTM B168 Hot Rolled Inconel 601 Stainless Steel Plates

Inconel 601 is a nickel-chromium alloy plate known for its high strength, heat resistance and corrosion resistance. This makes it suitable for many high-temperature applications.

ASTM B168 The excellent performance of Inconel 601 gaskets is mainly reflected in its characteristics. It has high tensile strength even at extremely high temperatures. Tensile strength means that it is not easily pulled apart. Inconel 601 can maintain its strength at high temperatures up to 2,000 degrees Fahrenheit (about 1047 degrees Celsius). It also has the characteristics of resistance to oxidation and corrosion. Oxidation means that it does not react with oxygen. Corrosion means that it does not react with other chemicals. This material is not easy to rust or degrade.

ASME SB168 Inconel 601 slit coils derive their properties from its mix of nickel, chromium, iron, and small amounts of other elements. Nickel gives it strength and ductility at high temperatures. Ductility means it can be formed and machined. Chromium helps it resist oxidation and corrosion.

This alloy is used to make parts that need to withstand extreme heat. For example, furnace parts. It can withstand the high temperatures inside a furnace without losing strength or corroding. ASME SB168 Inconel 601 hot rolled plate is also suitable for heat treating equipment. Heat treating is a process that uses precise heating and cooling to give metals specific properties. The alloy resists scaling and deformation at the high temperatures required for heat treating.

Other uses include annealing furnaces, reforming furnaces, and blasting nozzles. Annealing furnaces heat metal products to make them softer and easier to work with. Reforming furnaces use heat and steam to refine chemicals. Blasting nozzles direct the exhaust hot gases.

Inconel 601 alloy plate has excellent properties that make it well suited for extreme temperature environments. Its mix of metals gives it strength, corrosion resistance, and high-temperature resistance. Industries such as heat treating, chemical processing, and power generation rely on it to create durable components. This material is able to withstand damage that other metals may suffer.

ASME SB168 Plate Dimensions

Dimension (mm) Weight (kg)
1.6 1200 * 3048 14.4
0.9 * 1219 * 3048 8.1
3 * 1200 * 3000 27
0.7 * 1219 * 3048 6.3
1.2 * 1219 * 3048 10.8
3 * 1200 * 3000 27
0.5 * 1000 * 2000 4.5
3 * 1200 * 3000 27
2.0 * 1219 * 3048 18

ASTM B168 601 Inconel Plates Equivalent Grades

STANDARD UNS WERKSTOFF NR. AFNOR EN JIS BS GOST OR
Inconel 601 N06601 2.4851 NC23FeA NiCr23Fe NCF 601 NA 49 XH60BT ЭИ868

Inconel UNS N06601 Plates Chemical Composition

GRADE Ni C Fe Si Mn S Cu Cr
Inconel 601 58.0 – 63.0 0.10 max Balance 0.5 max 1.0 max 0.015 max 1.0 max 21.0 – 25.0

GNEE Group Factory Environment

ASTM B168 Hot Rolled Inconel 601 Steel Plates

ASTM B168 Hot Rolled Inconel 601 Stainless Steel Plates

GNEE Group Product Packaging

Hot Rolled Inconel 601 Stainless Steel Plates

ASTM B168 Hot Rolled Inconel 601 Stainless Steel Plates

FAQ

Q: Can provide OEM/ODM service?

A: Yes. Please feel free to contact us for more details discuss.

Q: How is your Payment Term?

A: Our usual payment methods are T/T, L/C, D/A, D/P, Western Union, Money Gram, payment methods can be negotiated and customized with customers.

Q: Can I get samples before order ?

A: Yes, of course.We can produce by your samples or technical drawings ;

Q: Can I go to your factory to visit?

A: Of course, we welcome customers from all over the world to visit our factory ;

Q:What are the shipping ports?

A:Under normal circumstances, we ship from Shanghai, Tianjin, Qingdao, Ningbo ports, you can choose other ports according to your needs.

Hot Tags: astm b168 hot rolled inconel 601 stainless steel plates, China astm b168 hot rolled inconel 601 stainless steel plates suppliers, duplex stainless steel alloy, duplex stainless steel product, duplex stainless steel grade, duplex stainless steel quotation, duplex stainless steel trader, duplex stainless steel purchase

Send Inquiry

whatsapp

Phone

E-mail

Inquiry