Duplex 2205 SS Flat Bar
video

Duplex 2205 SS Flat Bar

Duplex 2205 is a two-phase, ferritic, austenitic 22% chromium, 3% molybdenum, 5 to 6% nickel alloyed stainless steel. It is the most widely used duplex stainless steel grade and is characterized by high yield strength, double that of the standard austenitic stainless steel grades. It also demonstrates good fatigue strength, as well as outstanding resistance to stress corrosion cracking, crevice, pitting, erosion, and general corrosion in severe environments.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of duplex 2205 ss flat bar in China. If you're going to wholesale high quality duplex 2205 ss flat bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Duplex 2205 SS Flat Bar Description

Duplex 2205 Stainless Steel Rectangle Bar

GNEE STEEL GROUP supplies Duplex 2205 SS Flat Bar for you

 

Duplex 2205 flat steel is an austenitic-ferritic stainless steel used in corrosive environments and is resistant to localized corrosion such as pitting, crevice corrosion and stress corrosion cracking.

 

Dimensions of Duplex 2205 Flat Bar Available from GNEE STEEL

sizes in mm Size (inch) Thickness (in Inches) Thickness (mm)
22 7/8 2/3 – 5/7 17 & 18
25 1 3/16 – 4/5 5 to 20
30 1-3/16 3/16 – 4/5 5 to 20
32 1-1/4 1/4 – 4/5 6 to 20
35 1-3/8 3/16 – 3/16 5 to 20
40 1-4/7 3/16 – 1 5 to 25
45 1-7/9 3/16 – 1 5 to 25
47 1-6/7 2/3, 1 & 1-1/4 17,25 & 32
50 2 3/16 – 1-1/4 5 to 32
55 2-1/16 3/16 – 1 5 to 25
57 2-1/4 1-1/4 32
60 2-3/8 3/16 – 1-3/8 5 to 35
63 2-1/2 3/8 – 1-3/16 10 to 30
65 2-5/9 3/8 – 1-3/16, & 1-3/8 10 to 30 & 35
70 2-3/4 1/4 – 1, & 1-4/7 6 to 25 & 40
75 3 5/16 – 1 8 to 25
80 3-1/8 5/16 – 4/5 8 to 20
90 3-1/2 5/16- 4/5 8 to 20
100 4 5/16, 3/8, 1/2 8, 10, 12

The Application of Duplex 2205 SS Flat Bar :

  • Chemical processing, transport and storage – pressure vessels, tanks, piping, and heat exchangers
  • Oil and gas exploration and processing equipment – piping, tubing, and heat exchangers
  • Marine and other high chloride environments
  • Effluent scrubbing systems
  • Pulp and paper industry – digesters, bleaching equipment, and stock-handling systems
  • Cargo tanks for ships and trucks
  • Food processing equipment
  • Biofuels plants

 

Duplex 2205 SS Flat Bar Properties


2205 Duplex Stainless Steel Flat Bar Chemical Composition

C (Max) Mn (Max) P (Max) S (Max) Si (Max) CR NI MO Other Element
0.08 2.00 0.040 0.030 1.00 19.00/21.0 10.00/12.00 – –

 

Duplex 2205 Flat Bar Mechanical Properties

 

Grade YS (MPa) % Elongation UTS (MPa) Hardness(BHN)
31803 450 min. 25 min. 620 min. 293 max.

Duplex 2205 Stainless Steel  Flat Bar

stainless steel flat barCorrosion Resistance of Duplex 2205 Flat Bar:

Due to its high chromium, molybdenum, and nitrogen content, Duplex 2205 demonstrates superior corrosion resistant properties to 316 and 316L in most environments Chromium, molybdenum, and nitrogen content also provide high resistance to pitting and crevice corrosion, even in oxidizing and acidic solutions Resistant to chloride stress corrosion cracking and temperatures of up to about 302°F (150°C) .The presence of ferrite provides for good performance of Duplex 2205 in caustic environments.

Heat Resistance of Duplex 2205 Flat Bar:

Similar to other duplex stainless steels, Duplex 2205 has good oxidation resistance at high temperatures

Subject to embrittlement when exposed to temperatures above 572°F (300°C) even when exposed for short periods of time; Duplex 2205 is therefore not recommended for use above 572°F (300°C).

 

Customer Case

Customer Case 

Stainless Steel Flat Bar Customer Case

About US

 

 Rich Experience

GNEE Steel Group was founded in 2008 and has more than 10 years of experience in manufacturing steel.

 

 One-Stop Solution

GNEE Steel Group is a professional, one-stop supply chain enterprise for steel products, covering product research and development, sales, promotion, and providing professional services.

 

 Broad Market

The company's products are sold to Europe, Australia, and exported to more than 70 countries around the world. It has a total of more than 800 global cooperative enterprises, which include 15 shipbuilding companies, 143 engineering project companies, and 23 boiler machinery manufacturers.

 

 Delivery on Time

Our annual product sales volume is 1 million tons, our inventory is 200,000 tons, and our annual export volume has reached 80,000 tons, ensuring on-time delivery.

 

FAQ

 

Q:About Smls Pipe product prices?
A:Prices vary from period to period due to cyclical changes in the price of raw materials.

Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.

Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Q:Can you send samples?
A:Of course, we can send samples to all parts of the world, our samples are free, but customers need to bear the courier costs.

Q:About Duplex 2205 SS Flat Bar product prices?
A:Prices vary from period to period due to cyclical changes in the price of raw materials.

Hot Tags: duplex 2205 ss flat bar, China duplex 2205 ss flat bar suppliers, duplex stainless steel tee, duplex stainless steel acid resistance, duplex stainless steel use, duplex stainless steel wire, duplex stainless steel warranty, duplex stainless steel energy efficiency

Send Inquiry

whatsapp

Phone

E-mail

Inquiry