Stainless Steel Clad Plate(Hot Rolled)
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel clad plate(hot rolled) in China. If you're going to wholesale high quality stainless steel clad plate(hot rolled) made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hot rolling is a rolling process that involves rolling steel at temperatures above the recrystallization temperature of the steel (typically temperatures above 1700°F). When steel is above the recrystallization temperature, it can be easily formed and shaped, and the steel can be made into larger sizes. Hot rolled steel is usually cheaper than cold rolled steel because it is usually manufactured immediately and therefore does not need to be reheated (same as in the case of cold rolled steel). As the steel cools, it shrinks slightly, so there is less control over the size and shape of the stainless steel composite plate than with cold rolling.
Translated with DeepL.com (free version)




| Type | Stainless steel clad plate (hot rolled) |
| Thickness | Total thickness:5-50mm (cladding material thickness:1-10mm) |
| Width | Max:2500mm |
| Length | Max:15000mm |
| Finish | No.1 or as per your requirement |
| Standard | YB/T 4282-2012 |
| Materials | Base materials:carbon steel (Q235B, Q245R, Q345R),Cladding materials:stainless steel 300 series, duplex 2205. etc |
| Application | Petroleum, chemistry, electricity, paper making, alkali making, irrigation works, automobiles, salt, medicine, food and public facilities, For Kazakhstan Market |
| Package | Standard export sea-worthy package |
| Delivery Time | Usually 15-25 days after receiving the 30% deposit |
| Payment terms | TT, L/C, DP or Negotiable |
| Container Size | 20ft GP:5898mm(Length)x2352mm(Width)x2393mm(High)40ft GP:12032mm(Length)x2352mm(Width)x2393mm(High)40ft HC:12032mm(Length)x2352mm(Width)x2698mm(High) |
| Note | We are so able to produce other standard as per the clients' requirements. Just let us know. |
Electrical Engineering
For the steel liners used in sediment bottom holes, diversion bottom outlets, lock culverts and gates in hydropower industry, the basic requirements are high wear resistance, good impact resistance and adequate corrosion resistance. The liners are mainly used for silos, hoppers, chutes, dehydrators and other parts. Due to the more strictly enviromental protection policies, some air desulfurization projects are applied in order to reduce SO2 in the air. For those projects, the clad steel plates will become the preferred material of thermal power plants.
Pressure Vessels, Storage Tanks
Clad steel plates can reduce the consumption of high price metals or alloys, and reduce project cost significantly. Clad steel has excellent mechanical properties. The base material and cladding layer can form strongly metallurgical combination. Clad steel can be processed with a variety of hot pressing, bending, cutting, welding, etc. According to the applications of storage tanks, the base material can be selected from Q235B, Q345R carbon steels and other vessel steels. The cladding layer can be austenitic stainless steels such as 304, 316L, duplex stainless steel, and so on. The materials and the thicknesses can be freely combined to meet the property requirements of the different chemical storage tanks.
Petrochemical Industry
Clad steel has been widely used as containers, towers, heat exchangers, pipes in petrochemical equipment. For refining high-sulfur, high-salt and high acidity crude oil, clad steel can replace carbon steel and stainless steel used in the main refining equipment such as vacuum towers, absorption towers, fractionating towers, and the stabilizers, which increases corrosion resistance, heat resistance, as well as the service life of equipment. The advantages of clad steel are more obvious in the development of oil and natural gas fields with high H2 S, SO and nitrogen ions.
FAQ
1.Q: Are you a factory or trading company?
A: We are professional manufacturer, and our company also is a very professional a trade company for steel products.We can provide a wide range of steel products.
2.Q:What do your factory do regarding quality control?
A: We have obtained ISO, CE and other certifications. From materials to products, we check every process to maintain good quality.
3.Q: Can I get samples before order ?
A: Yes, of course. Usually our samples are free. we can produce by your samples or technical drawings.
4.Q:How do you make our business long-term and good relationship?
A:We keep good quality and competitive price to ensure our customers benefit ; We respect every customer as our friend and we sincerely do business and make friends with them. No matter where they come from.
Hot Tags: stainless steel clad plate(hot rolled), China stainless steel clad plate(hot rolled) suppliers, heat resistant alloy, equipment alloy, durable alloy, manufacturing alloy, machinery alloy, super alloy
You Might Also Like