Refractory 26 Tube
video

Refractory 26 Tube

Refractory 26 is Fe – Ni – Co – Cr based high temperature resistant, corrosion resistant alloy. It has excellent relaxation and creep resistance, and good plasticity under medium tem-perature.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of refractory 26 tube in China. If you're going to wholesale high quality refractory 26 tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Refractory 26 is Fe – Ni – Co – Cr based high temperature resistant, corrosion resistant alloy. It has excellent relaxation and creep resistance, and good plasticity under medium tem-perature.

 

Alloy R26 is Fe – NI – Co – Cr precipitation hardening type deformation of high temperature alloy, long-term use of C – 570 °C temperature range of 540 °C, the highest temperature can reach 677 C, add element of a Cr, mo alloy solid solution strengthening, high to low titanium, aluminum form y aging strengthening phase, while drilling elements made of titanium, aluminum solubility in the solid solution is reduced, prompted y phase precipitation amount increase, so as to improvel the thermal stability of y, reduce y 'phase of the stacking fault energy. The composite properties of the alloy are superior, with excellent tensile resistance, force relaxation and creep resistance, no notch sensitivity.

Common Trade Names:

Refractory 26 / GH2026 / Alloy R26 /W. Nr: 1.2888

Specifications:

AISI690

Alloy R26 Characteristic

The composite properties of the alloy are superior, with excellent tensile resistance, force relaxation and creep resistance, no notch sensitivity

Alloy R26 Chemical Composition

% Ni Cr Fe C Mn Si Ti Mo Co P S B Al
Min 35 16 - - 0.4 0.5 2.5 3 16 - - 0.001 -
Max 39 20 balance 0.08 1 1.5 3 3.4 22 0.03 0.03 0.01 0.3

Alloy R26 Physical Properties

Density Melting range
9.14g/cm³ 1300-1330°C

Alloy R26 Mechanical Properties (RT, Solution Annealed)

Tensile Strength (σb/MPa) Yield Strength (σp0.2/MPa) Elongation (σ5/%)
1000 550 15

product-720-720product-720-720product-720-720product-720-720

 

Alloy R26 Available Shape

Alloy R26 Size Range

»Round Bar & Square Bar & Hexagon Bar

● Diameter : φ8~φ300mm Length:10mm-6000mm

● Hot forging, Hot Rolling, Cold Drawing

● Bright Surface, Polished Surface, Black Surface

»Tube & Pipe:Seamless Tube& Welded Pipe

● Cold Drawing Seamless Pipe: φ1.0~φ220mm

● Hot Extrusion pipe: φ50~φ250mm

● Others : U Blend Tube and Elbow

»Hot Rolled Plate & Cold Rolled Sheet

● Cold Rolling Sheet Thickness: ≦2.0mm Width:≦1500m

● Hot rolling Plate Thickness: ≧4.0mm Width: ≦2500m

»Strip & Tape Ribbon

● Thickness: ≧ 0.01mm Width: 15mm-300mm

● Cold rolling BA Strip, Hard & Soft Condition

»Straight Length Wire & Spool Wire

● Welding Wire: φ 0.1mm~6.0mm Cut length Rod: φ1.0~φ8.0mm

● Package : 5-25kg/Spool or Box

 

FAQ

 

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Kazakhstan, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Hot Tags: refractory 26 tube, China refractory 26 tube suppliers, 2 4668 Nickel Alloy Steel Coil, Ni36CrTiAl Plate, Hastelloy C 22 Alloy Steel Flange, Hastelloy C276 ROUND BAR, Uns N06600 Alloy tubing, Cold Rolled Inconel 625 Alloy Seamless Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry