Nimonic 263 Alloy
video

Nimonic 263 Alloy

Nimonic 263 is an age-hardenable nickel-cobalt-chrome-molybdenum alloy which was designed to have excellent fabrication characteristics in the annealed condition but also very good aged strength properties. Alloy 263 is easier to form or weld than other materials such as Waspaloy or Rene 41 and exhibits excellent intermediate temperature ductility.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nimonic 263 alloy in China. If you're going to wholesale high quality nimonic 263 alloy made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Nimonic 263 is an age-hardenable nickel-cobalt-chrome-molybdenum alloy which was designed to have excellent fabrication characteristics in the annealed condition but also very good aged strength properties. Alloy 263 is easier to form or weld than other materials such as Waspaloy or Rene 41 and exhibits excellent intermediate temperature ductility.

 

Alloy 263 is strength at elevated temperature is not quite as high as materials such as HAYNES 282 alloy, Waspaloy alloy, or R-41 alloy. However, it is much easier to form or weld than Waspaloy alloy and R-41 alloy. Because HAYNES 282 alloy exhibits superior tensile, creep-rupture, and low cycle fatigue strength than HAYNES 263 alloy and has significantly greater fabricability than Waspaloy and R-41 alloys, it is replacing HAYNES 263 alloy in many applications. HAYNES 263 alloy is normally used for applications up to about 1650°F (900°C). Its oxidation resistance is comparable to that for other gamma-prime-strengthened superalloys. Alloy 263 can be welded using matching composition filler wire in both TIG and MIG forms

Common Trade Names:

Alloy 263 , Haynes C263 , Nimonic 263 , UNS N07263 , W.Nr: 2.4650 , Nicrofer 5120 CoTi

Specifications:

AMS 5872 Sheet, Plate and Strip /AMS 5886 Bar, Forgings, Rings /AFNOR NCK 20 D /AIR 9165 Sheet, Plate, Rod, Bar and Forgings /MSRR 7035 /MSRR 7036 /GE B50A774A

Nimonic 263 Characteristic

With very good aging strength characteristics,

Excellent manufacturing characteristics under annealing condition

Nimonic 263 Chemical Composition

% C Si Mn S Ag AI B Bi Co Cr Cu Fe Mo Pb Ti Ti+AI Ni
Min 0.04 – – – – 0.3 – – 19 19 – – 5.6 – 1.9 2.4 -
Max 0.08 0.4 0.6 0.007 0.0005 0.6 0.005 0.0001 21 21 0.2 0.7 6.1 0.002 2.4 2.8 balance

Nimonic 263 Physical Properties

Density Melting Point Coefficient of Expansion Modulus of Elasticity
8.36 g/cm3 1325 °C 10.6 μm/m• °C (20 – 100 °C) 222.5 kN/mm²
0.302 lb/in³ 2415 °F 5.7 x 10-6 in/in• °F (70 – 212 °F) 32270 ksi

Nimonic 263 Mechanical Properties

Material Temp °C Yield Strength 0.2% (Mpa) Tensile Strength (Mpa) Elongation % Hardness HB
Nimonic 263 Bar Solution Treated (AMS 5886/ BS HR10) RT - - - 248 max
Nimonic 263 Bar Heat Treated (AMS 5886 / BS HR10) RT 585 (typical) 1004 (typical) 45 -
Nimonic 263 Bar Heat Treated (AMS 5886/ BS HR10) 780 403 (min) 541 (min) 12 -
Nimonic 263 Sheet Solution Treated (AMS 5872 / BS HR206) RT - - - 22.5 max
Nimonic 263 Sheet Heat Treated (AMS 5872 / BS HR206 RT 580 (typical) 973 (typical) 39 -  
Nimonic 263 Sheet Heat Treated (AMS 5872 / BS HR206 780 403 (min) 541 (min) 9 -
product-720-720product-720-720product-720-720product-720-720

Nimonic 263 Heat Treatment

Alloy 263 is typically heat treated in two stages–solution treatment followed by an age hardening prior to service/fabrication.

Hot-Rolled sheet is normally given a solution treatment of 2100°F(1150°C), ½hr, water quenched or air cooled, followed by an aging of 1470°F(800°C), 8hrs, air cooled.

Cold-Rolled sheet and cold-drawn section(including tube) are given a solution treatment of 2100°F(1150°C), 3-10 minutes, FBQ or WQ, and then aged at 1470°F(800°C), 8hrs, AC.

Extruded/forged bars and section for forging or machining are usually solution treated at 2100°F(1150°C),1½-2½hrs, WQ, followed by an aging treatment of 1470°F(800°C), 8hrs, AC.

Nimonic 263 Available Shape

Nimonic 263 Size Range

Bars & Rods & Foring Ring /Flanges

Sheet & Plate

Strip & Coil

Welding Wire &Spring wire

Seamless Tube & Welded Pipe

 

FAQ

 

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Kazakhstan, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Hot Tags: nimonic 263 alloy, China nimonic 263 alloy suppliers, 2 4668 Nickel Alloy Steel Coil, Cold Rolled Inconel 625 Alloy Seamless Pipe, Uns N06600 Alloy tubing, Nickel Alloy Coil B2, Ni36CrTiAl Plate, Alloy Steel 600 plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry