Nickel 200/201 Alloy Plate
video

Nickel 200/201 Alloy Plate

Nickel 200/201 Alloy Plate is a commercially pure wrought nickel material with excellent mechanical properties and corrosion resistance. These alloys are used in a variety of industries due to their resistance to a wide range of corrosive environments, including acids, alkalies, and neutral salt solutions. Here's an overview:
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel 200/201 alloy plate in China. If you're going to wholesale high quality nickel 200/201 alloy plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Nickel 200/201 Alloy Plate is a commercially pure wrought nickel material with excellent mechanical properties and corrosion resistance. These alloys are used in a variety of industries due to their resistance to a wide range of corrosive environments, including acids, alkalies, and neutral salt solutions. 

 

Fabrication Data

Nickel 200 and 201 plate can be easily welded and processed by standard shop fabrication practices.

 

Hot Forming

Hot bending operations should be performed in the temperature range of 1600º to 2250ºF (870º to 1230ºC). In any operation, care should be taken to avoid heating Nickel 200 and 201 plate above the upper temperature limit of 2250ºF (1230ºC).

4 275

Cold Forming

Nickel 200 and 201 can be worked by any conventional cold-forming method. The forming characteristics are comparable to those of mild steel; however, because of the higher elastic limits of Nickel 200 and 201, greater power will be needed to perform the operations. Severe forming can be done manually but will require intermediate anneals to restore the alloy's softness.

 

Machining

Nickel 200 and 201 plate should be machined in the annealed condition whenever possible. These grades have the propensity to work harden, making it necessary to utilize low cutting speeds and requiring the cutting tool to stay engaged at all times. An adequate chip depth is important in order to avoid contact with the previously formed work-hardened zone. Liquid cold forming lubricants should be utilized to assure optimal heat dissipation.

200/201 alloy plates:

Category Nickel 200/201 Alloy Plate
Standards ASTM B162, ASME SB162
Thickness 0.1 mm to 12 mm
Width 600 mm to 2000 mm
Length Coil or cut-to-length options
Surface Finish Mill finish, 2B, custom finishes
Heat Treatment Annealed
Density 8.89 g/cm³ (0.321 lbs/in³)
Melting Range 1435–1446°C (2615–2635°F)
Modulus of Elasticity 205 GPa (29.7 x 10³ ksi)
Thermal Conductivity 66.5 W/m-°C at 100°C
Electrical Resistivity 0.096 µΩm at 20°C

4 166

Welding

Nickel 200 and 201 plate can be joined by a variety of welding procedures including inert gas and resistance welding. Welding practices are similar to those used to join austenitic stainless steels. Neither preheating nor post-weld heat treatments are usually required.

Hot Tags: nickel 200/201 alloy plate, China nickel 200/201 alloy plate suppliers, Cold Rolled Inconel 625 Alloy Seamless Pipe, Nickel Alloy Coil B2, Hastelloy C276 ROUND BAR, Uns N06600 Alloy tubing, Hastelloy C 22 Alloy Steel Flange, Ni36CrTiAl Plate