Ni36CrTiAl Plate
video

Ni36CrTiAl Plate

3J01 precision alloy is an iron-nickel-chromium austenite precipitation strengthening type with high elasticity alloy. After solution treatment, it has good plasticity, low hardness and easy processing and forming. After aging treatment after solid solution or cold strain, high mechanical properties and elastic properties are obtained.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ni36crtial plate in China. If you're going to wholesale high quality ni36crtial plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

3J01 precision alloy is an iron-nickel-chromium austenite precipitation strengthening type with high elasticity alloy. After solution treatment, it has good plasticity, low hardness and easy processing and forming. After aging treatment after solid solution or cold strain, high mechanical properties and elastic properties are obtained.

 

This type of alloy has the characteristics of high strength, high elastic modulus, small elastic aftereffect and hysteresis, weak magnetic properties, good corrosion resistance and thermal stability, and can be used at higher temperature and greater stress. Or work under corrosive media conditions. 3J01 alloy can work below 250ºC. This type of alloy can also be used at low temperatures (such as near -200°C).

Common Trade Names:

3J01 , Ni36CrTiAl , ЭИ702 , 36HXTЮ

3J01(Ni36CrTiAl) Characteristic

High elasticity, corrosion resistance, weak magnetic or non-magnetic.

3J01 Physical and Chemical Properties:

Coefficient Of Linear Expansion: The average linear expansion coefficient of the alloy is 20~100°c, 12~14*10-6 under the state of solution and aging
The Density: 8.0g/cm3 of 3J01 density cold strain aging state alloy.
Electrical Properties: ρ=1.02μΩ·m under cold deformation + aging condition.
Magnetic Properties: The magnetic susceptibility of 3J1 alloy in solution plus aging state is χm=(12.5 ~ 205)×10-11.
Chemical Properties: The alloy has good corrosion resistance to corrosive media such as nitric acid, phosphoric acid, sodium hydroxide, sulfurous petroleum, fuel oil and lubricating oil, as well as Marine and tropical climate conditions.

Product Description

3J01(Ni36CrTiAl) Chemical Composition

C Mn Si P S Ni Cr Mo Ti Al Fe
≤0.05 ≤1.00 ≤0.80 ≤0.020 ≤0.020 34.5~36.5 11.5~13.0 - 2.70~3.20 1.00~1.80 balance

3J01(Ni36CrTiAl) Mechanical Properties (Minimum value at 20℃)

Grade Condition Modulus of elasticity E/(N/m㎡) Tensile strength Rm N/m㎡ Hardness Hv
3J1 cold worked+Aged 186500-206000 ≥1200 400-480

3J01 Available Shape

3J01 Size Range

Bars & Rods & Foring Ring /Flanges

Sheet & Plate

Strip & Coil

Welding Wire &Spring wire

Seamless Tube & Welded Pipe

 

product-720-720product-720-720product-720-720product-720-720

 

3J1(Ni36CrTiAl) ApplicationsI

It is mainly used to make Make precision sensors, mechanical filter vibrators, tuning forks of frequency resonators, and reeds and diaphragms in resonant relays.

 

FAQ

 

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Kazakhstan, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Hot Tags: ni36crtial plate, China ni36crtial plate suppliers, Cold Rolled Inconel 625 Alloy Seamless Pipe, Alloy Steel 600 plate, 2 4668 Nickel Alloy Steel Coil, Nickel Alloy Coil B2, Uns N06600 Alloy tubing, Hastelloy C276 ROUND BAR