Monel K500 Alloy Metal Flange
Corrosion resistance
Precise dimensions
Can withstand high pressure and high temperature loads
Rust-proof surface
Smooth transition between flange thickness and pipe thickness
Ensures excellent stress distribution
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel k500 alloy metal flange in China. If you're going to wholesale high quality monel k500 alloy metal flange made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Monel K500 Metal Flange introduce
Monel K500 Alloy Flange


K500 Monel Flanges are a type of flange designed for high-pressure applications and commonly used in the oil and gas, chemical processing, marine and industrial piping industries. Monel K500 is an alloy composed of nickel, copper, iron/manganese, small amounts of niobium and aluminium. This combination provides excellent corrosion resistance at both high and low temperatures. The most common type of Monel K500 Flanges is weld neck flanges which are available in different pressure ratings such as 150 lb., 300 lb., 400 lb., 600 lb., 900 lb. & 1500lb (Class 150 to Class 1500).
Monel K500 Flanges Monel K500 flanges are made of a nickel-chromium alloy that has been carefully quenched and tempered. In this way, the tension on the flange surface is reduced and resistance to fatigue cracks caused by repeated bending or temperature fluctuations is enhanced.
Monel K500 flange alloy has a high strength-to-weight ratio and can be easily cast or forged and made into a variety of shapes. Due to its excellent corrosion and oxidation resistance, it is an ideal solution for industrial applications.
Equivalent Grades of Monel k500 flanges:
| STANDARD | WERKSTOFF NR. | UNS | JIS | AFNOR | BS | GOST | EN |
| Monel K500 | 2.4375 | N05500 | – | – | – | – | – |
Specifications of Monel k500 flanges:
Size |
: |
1/8″ NB TO 48″NB. |
Range |
: |
15 NB to 300 NB |
Specification |
: |
ANSI Flanges, ASME Flanges, BS Flanges, DIN Flanges, EN Flanges, etc. |
Standards |
: |
ASTM / ASME SB 564 / 160 / 472 |
Class |
: |
150#, 300#, 600#, 900#, 1500#, 2500#. PN6, PN10, PN16, PN25, PN40, PN64 etc. |
Grades |
: |
Monel 400 (UNS No. N04400), Monel K500 (UNS No. N05500). |
Chemical Composition of Monel k500 flanges:
| Monel K500 | Ni | Fe | C | Mn | Si | Cu | Al | Ti | S |
| 63.0 min | 05 – 2 | 0.25 max | 1.5 max | 0.5 max | 27.0 – 33.0 | 2.3 – 3.15 | 0.35 – 0.85 | 0.010 max |
K500 Alloy Metal Flange

GNEE Group Product Packaging
K500 Metal Flange


GNEE Company Environment
K500 Alloy Flange

FAQ
Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.
Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, Kazakhstan, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.
Q: Can you provide samples?
Answer: Yes. As long as you contact us, we can provide free small samples in stock. Customized samples will take about 5-7 days.
Hot Tags: Monel K500 Alloy Metal Flange, China Monel K500 Alloy Metal Flange suppliers, strong alloy, tough alloy, heat resistant alloy, special alloy, turbine alloy, machinery alloy
Previous
Monel End CapYou Might Also Like