Monel 502 R405 Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel 502 r405 pipe in China. If you're going to wholesale high quality monel 502 r405 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Monel 502 R405 Pipe
MONEL alloy 502 angle bars, MONEL alloy 502 flanges, Pipe Fitting, Steel Pipe, Heat Exchanger and Reducer, Gasket, Tee, Pipe Fitting, Tube Plate, have all specifications. With many yeas production experience, strict control MONEL alloy 502 chemical composition and MONEL alloy 502 mechanical properties.
R405 Monel Alloy is very similar for its greater sulfur content. Also has the same corrosion resistance and physical properties as the with a slightly different range of mechanical properties was developed for good.
Available forms are seamless pipe, welded pipe, seamless tube, welded tube, bar, wire, sheet, plate, forgings, pipe fittings and flanges.
| Trademark | GB | GOST | ASTM | UNS | DIN | W.Nr. | NF | BS |
| Monel R-405 | MCu-28-1.5-1.8 | НМЖМц28-2.5-1.5 | Monel R-405 | N04405 | NiCu30Fe | 2.4360 2.4361 |
Nu30 | Ni68Cu28Fe NA12 |
monel welding

Hot Tags: monel 502 r405 pipe, China monel 502 r405 pipe suppliers, special alloy, industrial alloy, machinery alloy, Monel K500 Nickel Alloy Pipe, engineering alloy, precision alloy