GH4169 alloy is a nickel-based high-temperature alloy precipitated and strengthened by body-centered square γ" and face-centered cubic γ' phases.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction
GH4169 4738 High Heat Stainless Steel Pipe Products Description

GH4169 4738 heat resistant alloy Pipe video

GNEE STEEL GROUP supplies GH4169 4738 High Heat Stainless Steel Pipe for you

 

Category Type Grade Designations
Grades Superalloys GH4169 China - GB , GB/T 14992 (2005) - Classification and designation for superalloys and high temperature intermetallic materials
GB/T 14994 (2008) - Cold brawn heat-resisting superalloy bars

 

Category Type Grade Designations
Grades Superalloys GH4738 China - GB ,
 
GH4169 4738 High Heat Stainless Steel Pipe chemical composition

GH4169 High Heat Stainless Steel Pipe chemical composition

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03    
Cr 17.0 21.0    
Mo 2.80 3.30    
Ni 50.0 55.0    
Al 0.20 0.60    
Nb 4.75 5.50    
Fe - Remainder    
Si - 0.35    
Mn - 0.35    
P - 0.015    
S - 0.015    
B - 0.006    

GH4738 High Heat Stainless Steel Pipe chemical composition

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.03 0.10    
Cr 18.0 21.0    
Mo 3.5 5.0    
Ni - Remainder    
Co 12.0 15.0    
Al 1.2 1.6    
Ti 2.75 3.25    
B 0.003 0.01    
Fe - 2.0    
Zr 0.02 0.08    

GH4169 4738 high heat stainless steel Pipe

GH4169 4738 heat resistant metals Pipe suppliersGH4169 4738 high heat resistant metals Pipe dealer

GH4169 alloy is a nickel-based high-temperature alloy precipitated and strengthened by body-centered square γ" and face-centered cubic γ' phases. It has good comprehensive properties in the temperature range of -253~700°C, and the yield strength below 650°C ranks among the highest deformation temperatures. It ranks first among alloys and has good fatigue resistance, radiation resistance, oxidation resistance, corrosion resistance, as well as good processing performance, welding performance and long-term structural stability. It can manufacture various parts with complex shapes and is used in aerospace, nuclear energy, In the petroleum industry, it has been widely used in the above temperature range.
GH738 is a nickel-based high-temperature alloy precipitated and hardened by the γ′ phase. It has good gas corrosion resistance, high yield strength and fatigue performance, good process plasticity, and stable structure. It is widely used in rotating parts of aerospace engines and the operating temperature is not higher than 815℃. It can produce cold-rolled and hot-rolled plates, pipes, strips, wires and forgings, castings and fasteners.

GNEE Group Factory Environment

GH4169 High Heat Stainless Steel oil pipe

GH4169 High Heat Stainless Steel oil pipe

GNEE Group Product Packaging

GH4738 High Heat Stainless Steel oil pipe

GH4738 High Heat Stainless Steel oil pipe

 

 

 

Product technology

High Heat Stainless Steel oil pipe

GH4169 4738 High Heat Stainless Steel Pipe

GH4169 4738 High Heat Stainless Steel Pipe

 

Customer Case

customer visit

GH4169 4738 High Heat Stainless Steel Pipe

 

Product packaging

GH4169 4738 Stainless Steel oil pipe

GH4169 4738 High Heat Stainless Steel Pipe

 

FAQ

Q: Do you provide samples? Is it free or extra?
A: Yes, we can provide samples for free without paying the shipping cost.

Q: What are your payment terms?
A: Payment <=1000USD, 50% in advance. Payment >=1000USD, 30% T/T in advance, balance before shipment. or negotiable

Q: About the product price of GH4169 4738 high temperature nickel alloys Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Contact Us

 

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

 

Hot Tags: GH4169 4738 High Heat Stainless Steel oil pipe, China GH4169 4738 High Heat Stainless Steel oil pipe suppliers

Send Inquiry

whatsapp

Phone

E-mail

Inquiry