High Strength Low Carbon Steel Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of high strength low carbon steel plate in China. If you're going to wholesale high quality high strength low carbon steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
High Strength Low Carbon Steel Plate
Product Description
Production Introduction

| Product Name | Hot Rolled steel plate |
| Grade | Q355B, S355 |
| Width | 1500mm-3800mm |
| Thickness | 4mm-800mm |
| Length | 5800mm-18000mm |
| Application | Steel Structure |
Production Line show

Export Processing Servcie
We can cut and slit the steel plate to meet client's customized requirement.

Product Application

Export packing and Logistics