Nickel 200 Alloy PIpe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel 200 alloy pipe in China. If you're going to wholesale high quality nickel 200 alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Nickel 200 Alloy pipe
The chemical composition Nickel 200 alloy is outlined in the following table.
|
(Ni) Nickel1 |
99.0 min |
|
(Fe) Iron |
0.40 max |
|
(Mn) Manganese |
0.35 max |
|
(Si) Silicon |
0.35 max |
|
(Cu) Copper |
0.25 max |
|
(C) Carbon |
0.02 max |
|
(S) Sulfur |
0.01 max |
Nickel 200 Alloy Application
Nickel Alloy 200 has many different industrial applications including:
Electronic Component
Electrical components
Heating element wire
Battery connections/terminals
Chemical processing
Aerospace parts
Food processing
Synthetic fiber processing
Nickel 200 Alloy Feature
Nickel 200 has the following key features:
Commercially pure nickel.
Resistant to various reducing chemicals and caustic alkalis.
Good magnetostrictive properties.
High electrical and thermal conductivity.
Good ductility and low work hardening rate.
Good solderability and weldability.