Nickel Based Alloy Hastelloy C276 Wire
video

Nickel Based Alloy Hastelloy C276 Wire

Hastelloy is a nickel-based corrosion-resistant alloy, which is mainly divided into two categories: nickel-chromium alloy and nickel-chromium-molybdenum alloy. Hastelloy has good corrosion resistance and thermal stability, and is mostly used in aviation, chemical fields, etc.   Hastelloy is composed of elements such as Ni, Cr, Mo, Fe, Si, etc. It is Ni-Mo series, Ni-Cr-Mo series and Ni-Si series corrosion-resistant and heat-resistant alloys in nickel-based alloys. Its density 9.2g/cm, melting point 1330-1380ºC, magnetic permeability≤1.001(ºC, RT).
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel based alloy hastelloy c276 wire in China. If you're going to wholesale high quality nickel based alloy hastelloy c276 wire made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy is a nickel-based corrosion-resistant alloy, which is mainly divided into two categories: nickel-chromium alloy and nickel-chromium-molybdenum alloy. Hastelloy has good corrosion resistance and thermal stability, and is mostly used in aviation, chemical fields, etc.


Hastelloy is composed of elements such as Ni, Cr, Mo, Fe, Si, etc. It is Ni-Mo series, Ni-Cr-Mo series and Ni-Si series corrosion-resistant and heat-resistant alloys in nickel-based alloys. Its density 9.2g/cm, melting point 1330-1380ºC, magnetic permeability≤1.001(ºC, RT).

H1976c1a871f1446e8f211352d6fc22e51png100x100xz

 Process Diameter Voltage Amperage Gas
TIG .045" (1.2mm) 13-16 80-110 100% Argon
1/16" (1.6mm) 14-18 90-130 100% Argon
3/32" (2.4mm) 15-20 120-175 100% Argon
1/8" (3.2mm) 15-20 150-220 100% Argon
MIG .045" (1.2mm) 28-32 180-220 75% Argon + 25% Helium
1/16" (1.6mm) 29-33 200-250 75% Argon + 25% Helium
SAW 3/32" (2.4mm) 28-30 275-350 Suitable Flux may be used
1/8" (3.2mm) 29-32 350-450 Suitable Flux may be used
5/32" (4.0mm) 30-33 400-550 Suitable Flux may be used

20231027152515

Q1. What are your company's main products

A1: Our main products are alloy materials, stainless steel, carbon steel, galvanized steel, aluminium products, etc.

Q2. How do you control quality ?

A2: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS Verified.

 

Q3. What are the advantages of your company ?

A3: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.

 

Hot Tags: nickel based alloy hastelloy c276 wire, China nickel based alloy hastelloy c276 wire suppliers, 2 4668 Nickel Alloy Steel Coil, Cold Rolled Inconel 625 Alloy Seamless Pipe, Alloy Steel 600 plate, Hastelloy C276 ROUND BAR, Monel 400 Alloy Steel Sheet, Hastelloy C 22 Alloy Steel Flange

Send Inquiry

whatsapp

Phone

E-mail

Inquiry