GH4080A 4098 composite pipe
video

GH4080A 4098 composite pipe

GH4080A is a high temperature alloy also known as Inconel 718. It is a nickel-based alloy with excellent high-temperature properties and corrosion resistance, making it widely used in the aerospace, petrochemical, nuclear industry and other high-temperature and high-pressure environments.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh4080a 4098 composite pipe in China. If you're going to wholesale high quality gh4080a 4098 composite pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

GH4080A 4098 composite pipe introduce

GH4080A 4098 composite pipe

GH4080A 4098 composite pipeGH4080A 4098 composite pipe

GH4060A high-temperature alloy, as an important high-performance material, has demonstrated its unique application value in many fields. Its excellent high-temperature resistance, high strength and good corrosion resistance make it irreplaceable in the aerospace field. In aircraft engines and rocket propulsion systems, GH4060A high-temperature alloy is widely used to manufacture key components such as combustion chambers and turbine blades. It can withstand the test of extreme high temperatures and complex stresses to ensure the safety and performance of aircraft.
GH4169 nickel-based alloy plate, with its unique chemical composition and phase composition, shows excellent high-temperature strength, corrosion resistance and processing performance, and is widely used in high-end industrial fields such as aerospace, nuclear energy, and petrochemicals. In practical applications, through precise heat treatment and processing technology, its performance potential can be further exerted to meet various stringent application requirements.

GH4080A Chemical Composition (Mass Fraction, wt.%)

Element Minimum (%) Maximum (%) Notes
C - 0.04 Carbon
Si - 0.10 Silicon
Mn - 0.80 Manganese
P - 0.020 Phosphorus
S - 0.015 Sulfur
Cr 18.00 21.00 Chromium
Ni Bal. - Nickel (Balance)
Mo - - Molybdenum (Not Specified)
V - - Vanadium (Not Specified)
Ta - - Tantalum (Not Specified)
W - 2.00 Tungsten
N - - Nitrogen (Not Specified)
Cu - 0.008 Copper
Co - - Cobalt (Not Specified)
Pb - - Lead (Not Specified)
B - - Boron (Not Specified)
Nb 1.00 1.80 Niobium
Al 1.80 2.70 Aluminum
Ti - - Titanium (Not Specified)
Other - - Trace elements (if any)

GH4098 Chemical Composition (Mass Fraction, wt.%)

Element Composition (wt.%) Notes
C ≤ 0.10 Carbon
Si ≤ 0.30 Silicon
Mn ≤ 0.30 Manganese
P ≤ 0.015 Phosphorus
S ≤ 0.015 Sulfur
Cr 17.5 – 19.5 Chromium
Ni Bal. (Balance) Nickel (Primary base)
Mo 3.5 – 5.0 Molybdenum
Co 5.0 – 8.0 Cobalt
Cu ≤ 0.07 Copper
Fe ≤ 3.0 Iron
Nb ≤ 1.5 Niobium
B ≤ 0.005 Boron
Ti 1.0 – 1.5 Titanium
Al 2.5 – 3.0 Aluminum
V - Vanadium (Not specified)
W 5.5 – 7.0 Tungsten
Ce ≤ 0.02 Cerium

GNEE Group Factory Environment

GH4098 composite pipe

GH4080A 4098 composite pipe

GNEE Group Product Packaging

GH4080A composite pipe

GH4080A 4098 composite pipe

FAQ

Q. How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Kazakhstan, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.

Hot Tags: GH4080A 4098 composite pipe, China GH4080A 4098 composite pipe suppliers, power generation alloy, Monel R405, strong alloy, corrosion resistant alloy, special alloy, advanced alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry