ASTM B160 UNS N02201Alloy Hex Bars
video

ASTM B160 UNS N02201Alloy Hex Bars

Name:ASTM B160 UNS N02201Alloy Hex Bars
Width:3mm-250mm
Surface:Bright
Density:8.9g/cm3
Transport Package:Carton or Wooden Case
Diameter (Od):Cold Drawn Bar: 4.76~120mm
Feature:High Corrosion Resistance, Low Density, Good Therm
Quality and Test:Hardness Test, Bending Test, Hydrostatic etc.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b160 uns n02201alloy hex bars in China. If you're going to wholesale high quality astm b160 uns n02201alloy hex bars made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

(Nickel 201, N02201) Pure Nickel Alloy Rod is a pure nickel alloy composed of trace elements such as manganese, copper and main body nickel. GNEE is a leading supplier and exporter of UNS N02201 Hexagonal Bars. We provide, Nickel 201 Square Bar, Nickel 201 Rectangular Bars, Nickel 201 Flat Bars, Nickel 201 Half Round Rods, Nickel 201 Threaded Rod, Nickel 201 Triangle Bars as per customer's requirements. The diameter range is usually between 6mm to 30mm.

 Nickel UNS N02201 Specification

ASTM B160 UNS N02201 Hex Bar Finish Specifications

Grades : Nickel 201 (UNS N02201)
Standards : ASTM, ASME and API
Specifications : ASTM B 160 / ASME SB 160
Size : 15NB to 150NB In
Length : 100 mm To 3000 mm Long & Above.
Form : Round, Square, Hex (A/F), Rectangle, Wire (Coil Form), Wire-mesh, Billet, Ingot, Forging Etc.
Finish : Bright, Polish & Black
 Alloys 201 Products Display

Nickel Alloy 201 Hollow Bar

product-800-400

Why choosing GNEE

GNEE is currently equipped with more than 10 finishing rolling and drawing production lines and 6 electrolysis equipment. It has introduced foreign advanced equipment such as bright annealing furnaces, straighteners, internal and external fine polishing machines, ECT eddy current and ultrasonic flaw detectors and other high-end instruments, and is equipped with high-grade dust-free room.

please contact us for a quote! ss@gneesteel.com

PRODUCTS TESTING

Nickel Alloy 201 High Temperature Pipe

Alloy 201 Black Bar Exporter

Alloy 201 Black Bar Exporter

 Alloy 201 bar Manufacturer

 Alloy 201 Bar Manufacturer

FAQ

Q.Are you a factory or a trading company?
A.We are a company with two mill and one warehouse,produce Stainless Steel/(Super)Duplex Steel/ Nickel Alloy seamless tube&pipes.
Q.Do you have any certificate?
A.We have approvals of ISO9001:2015,ISO14001:2015,ISO45001:2018, BV Ocean& Offshore Ship Classification Societies.

Q.How can you guarantee the quality of my goods?

A.We also accept third part inspection and EN10204.3.1B Mill test certificate for all materials.

Hot Tags: astm b160 uns n02201alloy hex bars, China astm b160 uns n02201alloy hex bars suppliers, Alloy Steel 600 plate, 2 4668 Nickel Alloy Steel Coil, Ni36CrTiAl Plate, Uns N06600 Alloy tubing, Cold Rolled Inconel 625 Alloy Seamless Pipe, Nickel Alloy Coil B2

Send Inquiry

whatsapp

Phone

E-mail

Inquiry