2J4 4J28 Nickel Based Alloy Pipe
video

2J4 4J28 Nickel Based Alloy Pipe

2J4 belongs to the iron-cobalt-vanadium series hysteresis alloy. This series of alloys is suitable for making high-efficiency hysteresis motor rotors.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 2j4 4j28 nickel based alloy pipe in China. If you're going to wholesale high quality 2j4 4j28 nickel based alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

2J4 4J28 Nickel Based Alloy Pipe

4J28 is a precision alloy composed of iron, nickel, cobalt and niobium. Its main features are high temperature stability and good corrosion resistance, so it is widely used in aviation, aerospace, manufacturing, medical equipment, electronic components and other fields.

In the aerospace field, 4J28 precision alloy is usually used to manufacture high-temperature components such as missiles, aircraft engines, and vibrators.

In manufacturing, it can be used as a basic material for high-precision mold manufacturing and as a manufacturing material for precision mechanical parts.

In the field of medical devices, 4J28 can be used as a solid support material to manufacture implantable devices, such as bone nails, bone plates, artificial joints, etc.

In the field of electronic components, 4J28 is often used to manufacture high-precision resistors, capacitors and inductors.

In addition to the above application fields, 4J28 precision alloy can also be used to manufacture superconducting materials, heat exchange tubes, high-speed train tracks, etc.

 

2J4 belongs to the iron-cobalt-vanadium series hysteresis alloy. This series of alloys is suitable for making high-efficiency hysteresis motor rotors. The operating temperature is high, and the alloy will not cause a reduction in magnetic properties in the range of +150~-140℃. Among various types of hysteresis alloys, 2J4 is the one that has been used for a longer time and has a larger dosage. After years of exploration and practice, the technology and production processes of our hysteresis alloy 2J4, 2J9, and 2J10 series products have become more perfect.
4J28 is a 4J28 precision alloy with abnormal thermal expansion characteristics, also known as 4J28 expansion alloy. It is widely used in the electronic industry, precision measurement tools, precision instruments, cryogenic engineering and other fields. Generally, metals and alloys expand after heating, and the expansion and temperature increase linearly. However, the bending point temperature of some alloy thermal expansion curves is much lower than the normal thermal expansion coefficient at the bending point. This phenomenon is called abnormal thermal expansion characteristics. . 4J28 expansion alloy is divided into low expansion alloy and fixed expansion alloy, the latter is also called sealing alloy.

Hot Tags: 2j4 4j28 nickel based alloy pipe, China 2j4 4j28 nickel based alloy pipe suppliers, Nickel Alloy Coil B2, Cold Rolled Inconel 625 Alloy Seamless Pipe, Monel 400 Alloy Steel Sheet, Uns N06600 Alloy tubing, Alloy Steel 600 plate, Ni36CrTiAl Plate